Freeze–thaw (F-T) is one of the principal perils afflicting concrete pavements. A remedial strategy used during construction encompasses the integration of hybrid fibers into the concrete matrix. An extant research gap persists in elucidating the damage mechanism inherent in hybrid steel fiber (SF)- and basalt fiber (BF)-reinforced concrete subjected to F-T conditions. This paper empirically investigated the durability performance of hybrid fiber-reinforced concrete (HFRC) subjected to F-T cycles. The impact of SF/BF hybridization on mass loss, abrasion resistance, compressive strength, flexural strength, damaged layer thickness, and the relative dynamic modulus of elasticity (RDME) was examined. The damage mechanism was explored using micro-hardness and SEM analysis. The results indicate that incorporating hybrid SF/BF effectively enhances the F-T resistance of concrete and prolongs the service life of concrete pavement. The mechanisms underlying these trends can be traced back to robust bonding at the fiber/matrix interface. Randomly dispersed SFs and BFs contribute to forming a three-dimensional spatial structure within the concrete matrix, suppressing the expansion of internal cracks caused by accumulated hydrostatic pressure during the F-T cycle. This research outcome establishes a theoretical foundation for the application of HFRC to concrete pavements in cold regions.
In the marine salt spray environment, steel fiber reinforced concrete (SFRC) structures are often subjected to accelerated durability degradation, primarily due to chloride-induced corrosion. To address this issue, polypropylene (PP) fibers were incorporated to partially replace steel fibers in the formulation of hybrid fiber reinforced concrete (HFRC), thereby enhancing its resistance to chloride corrosion. The results demonstrate that all HFRC mixtures achieved a compressive strength of approximately 65 MPa at 28 d. After 200 d of salt spray exposure, the compressive strength of the HFRC containing PP fibers decreased at a significantly slower rate than that of the control group (M0) incorporating sole steel fibers, with the former still meeting the high-strength concrete standard (>60 MPa). Regardless of the exposure duration to salt spray, the wave velocity of the HF series remained higher than that of M0. This suggests that the PP fibers play a significant role in preserving the matrix’s compactness, effectively mitigating deterioration caused by chloride corrosion. Furthermore, after 200 d of exposure, the peak chloride content, critical corrosion depth, and chloride diffusion coefficient of HF2 were 0.58%, 16 mm, and 1.24 × 10−12 m2/s, respectively, all of which were lower than those of the other specimens. This demonstrates that incorporating 0.3 vol% PP fibers most effectively enhances the chloride corrosion resistance of HFRC.