Friction stir welding (FSW) is well recognized as a very practical technology for joining magnesium alloys. Although, a large amount of progress have been made on the FSW of magnesium alloys, it should be emphasized that many challenges still remain in joining magnesium using FSW. In this article, we briefly review the background of friction stir welding of magnesium alloys, and then focus on the effects of the friction stir welding on the macrostructure, microstructure evolution, texture distribution, and the mechanical properties of the welding joints. The macro-defects in welds and their relationship to the welding parameters such as welding speed, rotation speed, and axial force were also discussed. The review concluded with some suggested methods improvement and future challenges related to FSW of magnesium alloys. The purpose of the present review paper is to fully understand the relationships between the microstructure and the properties, and then establish a global, state-of-the-art FSW of magnesium alloys.
In this paper, a 2D numerical model that is more physically realistic was established to simulate the complete process of Ti/Al explosive welding. Basing on the ANSYS/AUTODYN software package, the smoothed particle hydrodynamics (SPH) and arbitrary Lagrangian-Eulerian (ALE) were used for running this simulation. The numerical model can capture the typical physics in the explosive welding process, including the expansion of explosives, flyer plate bending, the impact of metal plates, jetting, and the wavy interface. The variable physical parameters during the explosive welding process were discussed. Most parts of the jet originated from the aluminum plate. According to the model, the jet velocity reached 7402 m/s. The pressure at the detonation point was too small to make the two plates to bond. The pressure could reach an order of magnitude of 107 kPa when the detonation energy tended to be stable and was far more than the yield strength of both materials, which resulted in an obvious narrow region of plastic strain emerging close to the collision zone. The signs of shear stresses between the two plates were the opposite. The interface morphology changed from straight to wave along the propagation of the detonation wave in the simulation, which was consistent with the experimental results.
A bimetal composite of 2205 duplex stainless steel and AZ31B magnesium alloy was cladded successfully through the method of explosive welding. The microstructural characteristics and mechanical properties of 2205/AZ31B bimetal composite are discussed. The interface of 2205/AZ31B bimetallic composite was a less regular wavy morphology with locally melted pockets. Adiabatic shear bands occurred only in the AZ31B side near explosive welding interface. The microstructure observed with EBSD showed a strong refinement near the interface zones. Line scan confirmed that the interface had a short element diffusion zone which would contribute to the metallurgical bonding between 2205 duplex stainless steel and AZ31B magnesium alloy. The value of micro-hardness near the bonding interface of composite plate increased because of work hardening and grain refinement. The tensile shear strength of bonding interface of 2205/AZ31B composite was 105.63 MPa. Tensile strength of 2205/AZ31B composite material was higher than the base AZ31B. There were two abrupt drops in stress in the stress–strain curves of the 2205/AZ31B composite materials.
13 May 2022 in Journal of Materials Engineering and Performance
The effects of element substitution and element doping on the magnetic properties and magnetocaloric effect of the LaFe11.5Si1.5 compound were investigated. The crystals of the LaFe11.5Si1.5, La0.8Nd0.2Fe11.5Si1.5, and LaFe11.5Si1.5C0.2 compounds all showed cubic NaZn13-type structures, but the lattice of the La0.8Nd0.2Fe11.5Si1.5 shrank and the lattice of the LaFe11.5Si1.5C0.2 expanded. All three compounds had the characteristic of first-order magnetic transition due to the obvious itinerant-electron metamagnetic (IEM) transition occurring above Curie temperature (TC). For the LaFe11.5Si1.5, La0.8Nd0.2Fe11.5Si1.5, and LaFe11.5Si1.5C0.2 compounds, the TC were approximately 194 K, 188 K, and 232 K, respectively. Meanwhile, the maximum magnetic entropy changes (−ΔSM) under a magnetic field change of 0–3 T were approximately 18.7 J/kg·K, 22.8 J/kg·K, and 16.4 J/kg·K, respectively. The TC was mainly affected by the lattice constant. Furthermore, the −ΔSM was mainly affected by the latent heat of the first-order magnetic transition.