Roll bonding (RB) of bimetal laminates is a solid phase method of bonding and has been widely used in the manufacturing of layered strips. This process is widely used for brazing sheet for automotive, aerospace, vessel, and electrical industries. In this study, 1-mm bimetallic aluminum 1050 and pure copper (Al/Cu) laminates were produced using the roll bonding (RB) process. The RB process was carried out with thickness reduction ratios of 10%, 20%, and 30%, separately. Particular attention was focused on the bonding of the interface between Al and Cu layers. The optimization of thickness reduction ratios was obtained for the improvement of the bond strength of bimetallic laminates during the RB process. Also, the RB method was simulated using finite element simulation in ABAQUS software. Finite Element (FE) simulation was used to model the deformation of bimetallic laminates for various thickness reduction ratios, rolling temperatures, and tensile stresses. Particular attention was focused on the rolling pressure of Al and Cu layers in the simulation. The results show that the stress distribution in the bimetal Al/Cu laminates is an asymmetrical distribution. Moreover, the bonding strength of samples was obtained using the peeling test. Also, the fracture surface of roll bonded samples around the interface of laminates after the tensile test was studied to investigate the bonding quality by scanning electron microscopy (SEM).
One of the popular techniques to fabricate metal matrix composites is the compo-casting process. The un-uniform spreading of reinforced subdivisions (particles) inside the metallic matrix and the lack of desirable mechanical properties of the final produced composites due to the low bonding strength among the metal matrix and reinforcement particles are the main challenges in this process. The warm accumulative press bonding (APB) technique was utilized as the supplementary technique to improve the mechanical and microstructural evolution of casted Al/TiC composite bars to remove these difficulties. So, using the tensile test, average Vickers micro hardness test, wear test and scanning electron microscopy (SEM), the microstructure evolution and mechanical properties of these composites have been considered vs. various WAPB steps. The SEM morphology of samples revealed that big titanium carbide clusters are broken and make a uniform distribution of titanium carbide particles at higher APB steps. It was shown that the cumulative forming steps of the APB process improved the mechanical properties of composites. In general, combining the compo-casting and APB process would result in making Al/TiC composites with high uniformity and good mechanical and microstructural properties.
18 December 2017 in International Journal of Materials Research
Composite materials and layered alloys have become an interesting topic in materials development. The roll bonding (RB) process as a solid phase method of bonding has been widely used in the manufacturing of layered strips. The poor bond strength is one of the major drawbacks of the RB process. In the present study, Pb particles were used to enhance the bond strength between aluminum strips as filler material. AA1050 particle-reinforced sheets with different contents of interlayer Pb particles were fabricated at various rolling temperatures and thickness reduction ratios. Effects of roll bonding parameters that create successful bonds such as amount of Pb particle content, plastic strain from rolling process and rolling temperature were investigated. The bond strength was evaluated by the peeling test. It was found that by increasing the rolling temperature, thickness reduction ratio and Pb content, successful bonds with higher strength were created. Scanning electron microscopy was utilized to characterize the peeled surface of AA1050/Pb samples.
22 May 2023 in Journal of Materials Engineering and Performance
In the present study, AA7075/Al2O3 composites have been fabricated via liquid metallurgy process. AA7075 alloy and Al2O3 particles were taken as the base matrix and reinforcements, respectively. Then, contents of 3 and 6 wt. % of Al2O3 subdivisions were added into the AA7075 matrix. To improve wettability and distribution, reinforcement particles were pre-heated to a temperature of 550°C for each composite sample. A hardened EN32 steel disc as the counter face was used to evaluate the wear rate pin-on-disc. The results showed that the wear rate of the AA/Al2O3 composites was smaller than that of the monolithic AA7075 samples. Finally, the worn surfaces of samples were investigated by SEM.