Nanoscale solute segregation to or near lattice defects is a coupled diffusion and trapping phenomenon that occurs in superalloys at high temperatures during service. Understanding the mechanisms underpinning this crucial process will open pathways to tuning the alloy composition for improving the high-temperature performance and lifetime. Here, we introduce an approach combining atom probe tomography with high-end scanning electron microscopy techniques, in transmission and backscattering modes, to enable direct investigation of solute segregation to defects generated during high-temperature deformation such as dislocations in a heat-treated Ni-based superalloy and planar faults in a CoNi-based superalloy. Three protocols were elaborated to capture the complete structural and compositional nature of the targeted defect in the alloy.
In this study, the effect of rhenium (Re) addition on microstructural evolution of a new low-density Co-Ni-Al-Mo-Nb based superalloy is presented. Addition of Re significantly influences the {\gamma}' precipitate morphology, the {\gamma}/{\gamma}' lattice misfit and the {\gamma}/{\gamma}' microstructural stability during long term aging. An addition of 2 at.% Re to a Co-30Ni-10Al-5Mo-2Nb (all in at.%) alloy, aged at 900{\deg}C for 50 hours, reduces the {\gamma}/{\gamma}' lattice misfit by {\approx} 40% (from +0.32% to +0.19%, measured at room temperature) and hence alters the {\gamma}' morphology from cuboidal to round-cornered cuboidal precipitates. The composition profiles across the {\gamma}/{\gamma}' interface by atom probe tomography (APT) reveals Re partitions to the {\gamma} phase (K_Re=0.34) and also results in the partitioning reversal of Mo to the {\gamma} phase (K_Mo=0.90) from the {\gamma}' precipitate. An inhomogeneous distribution of Gibbsian interfacial excess for the solute Re ({\Gamma}_Re, ranging from 0.8 to 9.6 atom.nm-2) has been observed at the {\gamma}/{\gamma}' interface. A coarsening study at 900{\deg}C (up to 1000 hours) suggests that the coarsening of {\gamma}' precipitates occurs solely by an evaporation--condensation (EC) mechanism. This is contrary to that observed in the Co-30Ni-10Al-5Mo-2Nb alloy as well as in some of the Ni-Al based and high mass density Co-Al-W based superalloys, where {\gamma}' precipitates coarsen by coagulation/coalescence mechanism with extensive alignment of {\gamma}' along directions as a sign of microstructural instability. The {\gamma}' coarsening rate exponent (K_r) and {\gamma}/{\gamma}' interfacial energy are estimated to be 1.41 x 10-27 m3/s and 8.4 mJ/m2, which are comparable and lower than Co-Al-W based superalloys.