Many researchers have been trying to improve rubber composites because they are commonly used in a wide range of applications. Incorporation of nano-fillers in a rubber matrix is the most acceptable way to improve the mechanical and electrical properties of rubber composites. A nanometer-sized filler, such as K0.15Cr0.02Ni0.83O (KCNO), has rarely been used to improve the properties of rubber composites. Epoxidized natural rubber (ENR) was chosen for blending with KCNO nanoparticles based on its polarity and chemical resistance. The aim of this work is to investigate the effects of filler loading (0.5, 1.5, and 5 phr) on the curing characteristics, dynamic mechanical, mechanical, morphological, and dielectric properties of rubber composites. From the results, rubber vulcanizates with 1.5 phr of KCNO as filler exhibit better tensile strength and 500% modulus compared to other ENR specimens containing KCNO. ENR containing 1.5 phr of KCNO also has a higher storage modulus (E′) and glass transition temperature (Tg). The results of a microstructural characterization on a sample containing 1.5 phr of KCNO show that the natural rubber matrix and KCNO are effectively dispersed, indicating that the rubber and KCNO are likely well-matched, therefore curing simultaneously and forming a continuous phase. Furthermore, ENR containing 1.5 phr of KCNO has a greater dielectric constant (12.87 at 5 kHz) than other samples.
The dielectric constant and mechanical properties of epoxidized natural rubber (ENR) were improved by forming composites with CeO2 and transition metal (TM) doped CeO2 nanoparticles (Ce0.8TM0.2O2, TM = Fe, Co, Ni, Cu, Mn and Zn). The CeO2samples and doped CeO2 nanoparticles were prepared using a co-precipitation method at room temperature and were calcined at 600 oC. The composites were prepared with 2 phr of CeO2, doped with CeO2 nanoparticles and referred to as CeO2@ENR, Fe-CeO2@ENR, Co-CeO2@ENR, Ni-CeO2@ENR, Cu-CeO2@ENR, Mn-CeO2@ENR and Zn-CeO2@ENR. CB@ENR composites were also prepared for comparison. The morphology, phase and valence states of prepared samples were characterized using transmission electron microscopy (TEM), X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), X-ray photoelectron spectroscopy (XPS). The samples exhibited XRD peaks and TEM-selected area electron diffraction corresponding to a face centered cubic CeO2 structure, confirming a single phase. They showed average crystallite sizes in the range of 10.5 ± 0.3 to 15.0 ± 1.4 nm. All TM-doped CeO2@ENR composites exhibited higher dielectric constants and lower dielectric losses at room temperature as a function of frequency than that of CB@ENR composites. A maximum value of ~392.6 at 102 Hz for the Cu-CeO2@ENR composite was shown. Additionally, this dielectric constant was about 3 and 4.7 times higher than those of CeO2@ENR and CB@ENR, respectively. Also, the breakdown strength of the Cu-CeO2@ENR nanocomposite was increased compared to CB@ENR. Furthermore, TM-doped CeO2 nanocomposites display increases in torque, higher 100% & 300% moduli and greater tensile strength caused by nano-filler affects. As a result, this research may open up new avenues for the development of insulating elastomers.