β-Ca3(PO4)2-type phosphors Ca9−xMnxEu(PO4)7 have been synthesized by high-temperature solid-phase reactions. The crystal structure of Ca8MnEu(PO4)7 was characterized by synchrotron X-ray diffraction. The phase transitions, magnetic and photoluminescence (PL) properties were studied. The abnormal reduction Eu3+ → Eu2+ in air was observed in Ca9−xMnxEu(PO4)7 according to PL spectra study and confirmed by X-ray photoelectron spectroscopy (XPS). Eu3+ shows partial reduction and coexistence of Eu2+/3+ states. It reflects in combination of a broad band from the Eu2+ 4f65d1 → 4f7 transition and a series of sharp lines attributed to 5D0 → 7FJ transitions of Eu3+. Eu2+/Eu3+ ions are redistributed among two crystal sites, M1 and M3, while Mn2+ fully occupies octahedral site M5 in Ca8MnEu(PO4)7. The main emission band was attributed to the 5D0 → 7F2 electric dipole transition of Eu3+ at 395 nm excitation. The abnormal quenching of Eu3+ emission was observed in Ca9−xMnxEu(PO4)7 phosphors with doping of the host by Mn2+ ions. The phenomena of abnormal reduction and quenching were discussed in detail.
A new series of Sr-based phosphates, Sr9−xMnxEu(PO4)7, were synthesized using the high-temperature solid-state method in air. It was found that these compounds have the same structure as strontiowhitlockite, which is a β-Ca3(PO4)2 (or β-TCP) structure. The concentration of Mn2+ ions required to form a pure strontiowhitlockite phase was determined. An unusual partial reduction of Eu3+ to Eu2+ in air was observed and confirmed by photoluminescence (PL) and electron spin resonance (ESR) spectra measurements. The PL spectra recorded under 370 nm excitation showed transitions of both 4f5d–4f Eu2+ and 4f–4f Eu3+. The total integral intensity of the PL spectra, monitored at 395 nm, decreased with increasing Mn2+ concentration due to quenching effect of Eu3+ by the Mn2+ levels. The temperature dependence of Eu2+ photoluminescence in a Sr9−xMnxEu(PO4)7 host was investigated. The conditions for the reduction of Eu3+ to Eu2+ in air were discussed.
To establish the connection between structure, conductivity and luminescence properties, the Na3Sc2−xRx(PO4)3 (R = Eu, Tb, Dy; 0 ≤ x ≤ 0.2) compounds have been studied. Solid solutions with a NASICON-type structure were formed at 0 ≤ x ≤ 0.1.
To establish the connection between the structure and luminescence properties in NASICON type structure, Na 3.6 Lu
1.8−
x (PO 4 ) 3 : x Eu 3+ compounds have been studied. The enhanced thermal stability of the Eu 3+ emission was obtained at Eex = 3.23 eV.
The decay kinetics of Gd3Al2Ga3O12:Ce3+ single crystal luminescence were studied under dense laser excitation. It was shown that the decay times as well as the intensity of Ce3+ luminescence depend on the excitation density. The observed effects were ascribed to the interaction between excitons as well as to the features of energy transfer from the excitons to Ce3+. The numerical simulation of the experimental results was performed for justification of the proposed model.
The structural features of a series of ZnxMg1–xWO4 mixed crystals (x = 0, 0.26, 0.41, 0.68, or 1) have been investigated using X-ray diffraction analysis and Raman spectroscopy; the luminescence properties of the grown crystals have also been studied. The dependence of the unit-cell volume on the substitution-cation concentration x is determined. It is shown that the geometric parameters of WO6 octahedra are independent of the ratio of Zn and Mg atomic concentrations in crystals. Consistency between the luminescence and structural properties of ZnxMg1–xWO4 crystals is established.