Fe–Ni alloy nanowires are widely used in high-density magnetic memories and catalysts due to their unique magnetic and electrochemical properties. Understanding the deformation mechanism and mechanical property of Fe–Ni alloy nanowires is of great importance for the development of devices. However, the detailed deformation mechanism of the alloy nanowires at different temperatures is unclear. Herein, the deformation mechanism of Fe–Ni alloy nanowires and their mechanical properties were investigated via the molecular dynamics simulation method. It was found that the local atomic pressure fluctuation of the Fe–Ni alloy nanowire surface became more prominent with an increase in the Ni content. At low temperature conditions (<50 K), the plastic deformation mechanism of the Fe–Ni alloy nanowires switched from the twinning mechanism to the dislocation slip mechanism with the increase in the Ni content from 0.5 at% to 8.0 at%. In the temperature range of 50–800 K, the dislocation slip mechanism dominated the deformation. Simulation results indicated that there was a significant linear relationship between the Ni content, temperature, and ultimate stress in the temperature range of 50–800 K. Our research revealed the association between the deformation mechanism and temperature in Fe–Ni alloy nanowires, which may facilitate new alloy nanowire designs.
The formation of BCC structure in the melt was the key in TiAl crystalline nucleation, and liquid TiAl alloy completely crystallized at the quenching rate of 0.02 K ps−1.
In this paper, the processes of rapid solidification in TiAl was investigated by molecular dynamics simulations. The structure transformation which occurs during solidification is described by internal energy, radial distribution functions, Honeycutt-Anderson pair analysis technique, mean square displacement and simulation of powder X-ray diffraction patterns. The effects of different cooling rates, 50–0.005 K ps−1, on the amorphous structure formation and crystallization of liquid TiAl are simulated. The results show that an amorphous phase can be obtained when the cooling rate is not less than 0.02 K ps−1, and γ-TiAl + α2-Ti3Al mixed phases can be formed when the cooling rate is 0.01 K ps−1.
22 February 2022 in Journal of the European Ceramic Society