The inadequate hole injection limits the efficiency and lifetime of the blue quantum dot light‐emitting diodes (QLEDs), which severely hampers their commercial applications. Here a new discotic molecule of 3,6,10,11‐tetrakis(pentyloxy)triphenylene‐2,7‐diyl bis(2,2‐dimethylpropanoate) (T5DP‐2,7) is introduced, in which the hole transport channels with superior hole mobility (2.6 × 10–2 cm2 V–1 s–1) is formed by stacking. The composite hole transport material (HTM) is prepared by blending T5DP‐2,7 with the cross‐linked 4,4′‐ bis(3‐vinyl‐9H‐carbazol‐9‐yl)‐1,1′biphenyl (CBP‐V) which shows the deep highest occupied molecular orbital energy level. The increased hole mobility of the target composite HTM from 10–4 to 10–3 cm2 V–1 s–1 as well as the stepwise energy levels facilitates the hole transport, which would be beneficial for more balanced carrier injection. This composite hole transport layer (HTL) has improved the deep‐blue‐emission performances of Commission International de I'Eclairage of (0.14, 0.04), luminance of 44080 cd m−2, and external quantum efficiency of 18.59%. Furthermore, when L0 is 100 cd m−2, the device lifetime T50 is extended from 139 to 502 h. The state‐of‐the‐art performance shows the successful promotion of the high‐efficiency for deep blue QLEDs, and indicates that the optimizing HTL by discotic molecule stacking can serve as an excellent alternative for the development of HTL in the future.
12 December 2018 in Journal of Materials Chemistry A
Room-temperature-processed C60 single-crystalline nanoparticles were employed as a high-performance organic electron-selective scaffold for both rigid and flexible perovskite solar cells.
The coffee-ring effect and material aggregation are main obstacles to obtaining high-performance small-molecule hole-transport layers by non-bank inkjet printing for organic light-emitting diodes (OLEDs). In this paper, a binary solvent ink system of cyclohexane-dipropylene glycol methyl ether (CYC–DGME) was constructed for the cross-linkable hole-transport material N,N′-di-p-tolyl-N,N′-bis(4-vinylphenyl)-[1,1′-biphenyl]-4,4′-diamine (V-p-TPD). The coffee-ring effect during film formation was eliminated by adjusting the solvent ratio and printing conditions. Furthermore, N2,N2,N7,N7-tetrakis(4-(3,6-di-tert-butyl-9H-carbazol-9-yl)-phenyl)-9,9-dimethyl-9H-fluoren-2,7-diamine (p-BCz-F) was used as the auxiliary hole-transport component. With V-p-TPD/p-BCz-F = 8 : 2 and CYC/DGME = 7 : 3, non-bank inkjet printing and thermal cross-linking produced an alloy-like hole-transport layer film with a low surface roughness (RMS = 1.23 nm) and excellent resistance to solvents. The target green phosphorescent OLEDs were qualified with an enhanced maximum current efficiency, external quantum efficiency and lowered turn-on voltage of 55.47 cd A−1, 15.44% and 3.18 V, respectively, which represents a state-of-the-art record among OLEDs based on inkjet-printed HTLs. This result provides an effective and unique approach for the facile preparation of highly efficient OLED display devices by inkjet printing.