With extensive first-principles density-functional calculations, we construct a three-dimensional compositional phase diagram of Ba1−xCaxZryTi1−yO3 (BCZT) with the Ca and Zr content in the ranges of 0 ≤ xCa ≤ 0.2 and 0 ≤ yZr ≤ 1. Our calculations show that, when the Zr content increases, the difference in energy and difference in the structural parameters of the cubic, tetragonal, orthorhombic, and rhombohedral phases of BCZT are reduced. Eventually, all four phases merge into a multiphase with coexisting cubic structures (MPCCS) under Zr-rich conditions, indicating that BCZT undergoes phase transition from a normal ferroelectric (NFE) to a relaxor ferroelectric (RFE), consistent with experimental observations. The 3D diagram shows that the regions of merged and separated energy surfaces correspond to the regions of the RFE and NFE, respectively, which suggests that a MPCCS corresponds to a RFE. In addition, with the MPCCS model and Landau–Devonshire theory, we provide an interpretation of the high electromechanical properties of the BCZT relaxor ferroelectric and apply it to the classical local random field and micro–macro domain transition models.
2 November 2016 in Journal of the American Ceramic Society
Ab initio density-functional theory and thermodynamics calculations are combined to establish a microscopic mechanism for the oxidation of the α2-Ti3Al(0001) surface. The surface energies as functions of the chemical potentials, as well as structural relaxations and electronic densities of states, are determined. The surface phase diagram (SPD) of the α2-Ti3Al(0001) systems with different defects and at various oxygen coverages is constructed. It is found that the Al antisite defect prefers to segregate on the α2-Ti3Al(0001) surface and oxygen adsorption enhances the segregation with the formation of the surface with three Al antisites per unit surface cell (i.e. the top surface layer is full of Al atoms) at the initial stage of oxidation, accounting for the aluminum selective oxidation observed experimentally. After the initial stage of oxidation, the O–α2-Ti3Al(0001) system manifests itself with a non-uniform double-phase SPD, suggesting the competition between oxidations of the Al and Ti elements in the oxidation process. This result explains the experimentally observed second regime of oxidation in which both metal elements are oxidized.