1 February 2014 in Dental Materials
Verified
Journal Article
Closed access
KZKe Zhao
Ke Zhao
YWYa-Ru Wei
Ya-Ru Wei
YPYu Pan
Yu Pan
XZXin-Ping Zhang
Xin-Ping Zhang
MSMichael V. Swain
Michael V. Swain
PGPetra C. Guess
Petra C. Guess

1 April 2016 in Journal of Dentistry
Verified
Journal Article
Closed access
YWYa-Ru Wei
Ya-Ru Wei
XWXiao-Dong Wang
Xiao-Dong Wang
QZQin Zhang
Qin Zhang
XLXiang-Xia Li
Xiang-Xia Li
MBMarkus B. Blatz
Markus B. Blatz
KZKe Zhao
Ke Zhao

1 November 2016 in The Journal of Prosthetic Dentistry
Verified
Journal Article
Closed access
LZLi Zhao
Li Zhao
YJYu-Tao Jian
Yu-Tao Jian
XWXiao-Dong Wang
Xiao-Dong Wang
KZKe Zhao
Ke Zhao

1 January 2019
Verified
Journal Article
Closed access
XWXiaodong Wang
Xiaodong Wang
XSXin Shu
Xin Shu
YZYingbin Zhang
Yingbin Zhang
BYBin Yang
Bin Yang
YJYutao Jain
Yutao Jain
KZKe Zhao
Ke Zhao

14 June 2021 in Journal of Materials Science: Materials in Medicine
Verified
Journal Article
Open access
PDF file
YYYi-Tong Yao
Yi-Tong Yao
YYYue Yang
Yue Yang
QYQi Ye
Qi Ye
SCShan-Shan Cao
Shan-Shan Cao
XZXinping Zhang
Xinping Zhang
YJYutao Jian
Yutao Jian
To find out the optimal porosity and pore size of porous titanium (Ti) regarding the cytocompatibility and osteogenic differentiation. Six groups of porous Ti samples with different porosities and pore sizes were fabricated by the powder metallurgy process. The microstructure and compressive mechanical properties were characterized. The cytocompatibility was examined by a series of biological tests as protein absorption with BCA assay kit, cell attachment with laser scanning confocal microscopy and vinculin expression, cell proliferation with CCK-8 assay. Cell differentiation and calcification were detected by qPCR and Alizarin Red S dying respectively. Pores distributed homogeneously throughout the porous Ti samples. The compressive test results showed that Young’s modulus ranged from 2.80 ± 0.03 GPa to 5.43 ± 0.34 GPa and the compressive strength increased from 112.4 ± 3.6 MPa to 231.1 ± 9.4 MPa. Porous Ti with high porosity (53.3 ± 1.2%) and small pore size (191.6 ± 3.7 μm) adsorbed more proteins. More MC3T3-E1 cells adhered onto dense Ti samples than onto any other porous ones already after culture and no difference was identified within the porous groups. The porous structure of porous Ti with a porosity of 53.3 ± 1.2% and an average pore size of 191.6 ± 3.7 μm facilitated cell differentiation and calcification. Small pores were not beneficial to the osteo-initiation at the very beginning. Porous Ti with a porosity of 53.3 ± 1.2% and an average pore size of 191.6 ± 3.7 μm fabricated by powder metallurgy process showed the expected mechanical property and improved osseointegration as implants in dental treatment.

5 June 2015 in PLOS ONE
Verified
Journal Article
Open access
PDF file
YJYu-Tao Jian
Yu-Tao Jian
YYYue Yang
Yue Yang
TTTian Tian
Tian Tian
CSClark Stanford
Clark Stanford
XZXin-Ping Zhang
Xin-Ping Zhang
KZKe Zhao
Ke Zhao
Five types of porous Nickel-Titanium (NiTi) alloy samples of different porosities and pore sizes were fabricated. According to compressive and fracture strengths, three groups of porous NiTi alloy samples underwent further cytocompatibility experiments. Porous NiTi alloys exhibited a lower Young’s modulus (2.0 GPa ~ 0.8 GPa). Both compressive strength (108.8 MPa ~ 56.2 MPa) and fracture strength (64.6 MPa ~ 41.6 MPa) decreased gradually with increasing mean pore size (MPS). Cells grew and spread well on all porous NiTi alloy samples. Cells attached more strongly on control group and blank group than on all porous NiTi alloy samples (p < 0.05). Cell adhesion on porous NiTi alloys was correlated negatively to MPS (277.2 μm ~ 566.5 μm; p < 0.05). More cells proliferated on control group and blank group than on all porous NiTi alloy samples (p < 0.05). Cellular ALP activity on all porous NiTi alloy samples was higher than on control group and blank group (p < 0.05). The porous NiTi alloys with optimized pore size could be a potential orthopedic material.