The effect of fluid media on material removal and subsurface defects evolution in nano-cutting process of single-crystal copper is investigated by means of molecular dynamics simulation. In this paper, the removal mechanism of the chip and formation mechanism of machined surface are investigated by analyzing the atomic migration and dislocation evolution of workpiece during nano-cutting process with the use of aqueous media. The distribution of temperature and subsurface defect crystal structural transformation are investigated, which are analyzed by centro-symmetry parameter and common neighbor analysis methods. The results show that the workpiece material is removed by the extrusion shearing action of the cutting tool. The lubrication of the aqueous media can reduce the cutting force and lower the height of cutting chip. Particularly, the cooling action of the fluid media results in the formation of a typical defect “similar-to-grain boundary” in subsurface of the workpiece. And the temperature of workpiece has a distinct decrease during nano-cutting process with the use of fluid media.
Subsurface defects have a significant impact on the precision and performance of nano-structures. In this paper, molecular dynamics simulation of nano-indentation is performed to investigate the effect of machining-induced subsurface defects on dislocation evolution and mechanical properties of materials, in which the specimen model with subsurface defects is constructed by nano-cutting conforming to reality. The formation mechanism of subsurface defects and the interaction mechanism between machine-induced defects and dislocation evolution are discussed. The hardness and Young’s elastic modulus of single crystal copper specimens are calculated. The simulation results indicate that there exist stable defect structure residues in the subsurface of workpiece, such as atomic clusters, stacking fault tetrahedral, and stair-rod dislocations. Secondary processing of nano-indentation can restore internal defects of the workpiece, but the subsurface damage in the secondary processing area is aggravated. The nano-indentation hardness of specimens increases with the introduction of subsurface defects, which results in the formation of work-hardening effect. The existence of subsurface defects can weaken the ability of material to resist elastic deformation, in which the mutual evolution between dislocations and subsurface defects plays an important role.
18 July 2024 in Journal of Molecular Graphics and Modelling
A sequentially coupled multi-phase thermo-mechanical model for laser powder bed fusion (LPBF) of Al-based composites reinforced by 1 wt.% random TiB2 micron particles was established. Due to the remarkable difference in thermophysical properties, the maximum thermal stress was predicted at the TiB2/Al matrix interface and formed at the liquid–solid transition stage. Meanwhile, complicated evolution curves of temperature, strain, and strain rate were predicted with the laser moving time during the solidification stage. To evaluate the interface cracking susceptibilities of micron-TiB2/AlSi10Mg composites, the flow stress of the matrix was calculated, instead of ultimate tensile strength, based on the physical constitutive relationship. From the comparison between the calculated flow stress and the simulated Von Mise equivalent stress, it was found that an increase in TiB2 particle size was inclined to induce a larger interfacial stress than the calculated flow stress, therefore increasing the interfacial crack tendency, which was also effectively verified by the experimental results.
Laser Powder Bed Fusion (LPBF) technology exhibits significant advantages in the manufacturing of components with high dimensional accuracy and intricate internal cavities. However, due to the inherent room-temperature brittleness and high-temperature gradient induced by the laser forming process, the LPBF fabrication of γ-TiAl alloy is often accompanied by the initiation and propagation of defects. The aim of this study is to investigate the forming process of γ-TiAl alloy by the LPBF method through molecular dynamics simulation, and to explain the microparticle arrangement and displacement evolution of the melting and crystallization processes, thus elucidating the link between the variations in the laser process parameters and defect generation during microscopic laser heating. The results show that during the melting process, the peaks of the radial distribution function (RDF) decrease rapidly or even disappear due to laser heating, and the atomic disorder is increased. Although subsequent cooling crystallization reorders the atomic arrangement, the peak value of the RDF after crystallization is still 19.3% lower than that of the original structure. By setting different laser powers (200–800 eV/ps) and scanning speeds (0.2–0.8 Å/ps), the effects of various process parameters on microforming and defect evolution are clarified. When the laser power increases from 200 to 400 eV/ps, the stable value of atomic displacement rises from 6.66 to 320.87, while it rises from 300.54 to 550.14 when the scanning speed is attenuated from 0.8 to 0.4 Å/ps, which indicates that, compared with the scanning speed, the atomic mean-square displacements are relatively more sensitive to the fluctuation of laser power. Dislocation analysis reveals that a higher laser power significantly increases the cooling rate during the forming process, which further aggravates the generation and expansion of dislocation defects.
Shoulder fillets are widely used in the structural optimization design of metal dampers. However, the plastic deformation property of dampers affected by stress concentration, owing to different fillets, has not been explored in-depth. In this study, two typical metal damper materials with different plastic deformation, i.e., ordinary steel SS400 and low-yield-strength steel LYS160, were investigated. The strengthening effect of fillets under different loading is evaluated by comparing the mechanical properties of different fillet heights. Furthermore, the effect of the stress concentration caused by different fillet shapes, based on the failure mode of materials, is discussed. Subsequently, the fatigue degradation effect under the reciprocating shear loading is studied. Based on a series of studies on the deformation properties of fillets in different ductile materials, the basis for the structural optimization design under plastic deformation is provided.