Doping can alter certain electronics, including the thermoelectric properties of an organic semiconductor. These alterations may enable viable tunable devices that could be useful in temperature sensing for autonomous controls. Here, we demonstrate a dual-modulation organic field-effect transistor (OFET) where temperature can modulate the current-voltage characteristics of the OFET and gate voltage can modulate the thermoelectric properties of the active layer in the same device. Specifically, Poly(3-hexylthiophene-2,5-diyl) (P3HT) was utilized as the host p-type semiconducting polymer, and iodine was utilized as the thermoelectric minority dopant. The finished devices were characterized with a semiconductor analyzer system with temperature controlled using two thermoelectric cooling plates. The FETs with iodine doping levels in the range of 0.25% to 0.5% mole ratio with respect to the P3HT exhibit the greatest on/off ratios. This study also observed that P3HT thin film samples with an intermediate iodine doping concentration of 0.25% mole ratio exhibit an optimal thermoelectric power factor (PF).
Doping can alter the electronic and thermoelectric attributes of an organic semiconductor system. These alterations can enable viable tunable devices that have applications in temperature sensing for environmental controls. Here we demonstrate a dual-modulation organic field-effect transistor (OFET) where temperature effectively modulates the current-voltage characteristics of the OFET and gate voltage modulates the thermoelectric properties of the active layer. Poly(3-hexylthiophene-2,5-diyl) (P3HT) was utilized as the host donor polymer, iodine was utilized as the dopant acceptor molecule Finished devices were characterized by a semiconductor analyzer system with temperature controlled by two thermoelectric cooling plates. The doping of iodine in the range of 0.25% to 0.5% mole ratio with respect to the P3HT exhibited the greatest on-off ratio of the investigated dopant concentrations. Iodine doping concentrations of 0.5% mole ratio or less can greatly improve the thermoelectric properties of a binary P3HT-based system and the current-voltage performance of the dual-modulation device.