During the last decade, considerable progress has been made in understanding the properties and behavior of the vacancy V and self-interstitial I in silicon (Si) and germanium (Ge) crystals. This is to a large extent due to the maturing of density functional theory (DFT) calculation techniques and the increase of computing power enabling to calculate not only the formation and migration energies of V and I, but also the interaction with impurities and with crystal surfaces. Furthermore, the impact of internal and external stress on formation and migration enthalpies of both intrinsic point defects has been clarified recently. In this paper an overview is given on recent assessments on the properties of intrinsic point defects in Si and Ge, and on the useful application of DFT calculations for the control and engineering of intrinsic point defects in Si and Ge single crystal growth from a melt.
Very recently, first experimental evidence was published that the compressive thermal stress near the melt/solid interface makes a growing 300 mm diameter Czochralski Si crystal more vacancy-rich. The purpose of this letter is to explain these experimental results quantitatively by determining the dependence of the formation enthalpies of the vacancy and the self-interstitial on compressive plane stress using density functional theory based calculations. It is found that compressive plane stress gives a higher stress dependence of the so-called “Voronkov criterion” compared to the isotropic stress. In most of the central region of a growing crystal, the dominant component of the thermal stress near the melt/solid interface is compressive plane stress. The calculated plane stress dependence is in excellent agreement with the published experimental values and should be taken into account in the development of pulling processes for the mass-production of 450 mm diameter defect-free Si crystals.
To explain and engineer intrinsic point defect behavior in large-diameter single crystal Si grown using the Czochralski (CZ) method, a unified model valid for all pulling processes, crystal resistivities, and electrically inactive impurity concentrations that couples the effects of thermal stress, dopants, and interstitial oxygen (Oi) atoms is needed. We determined the thermal equilibrium concentration of intrinsic point defects (vacancy V and self-interstitial Si I) in CZ-Si crystal as functions of thermal stresses, type and concentration of dopant, and the concentration of Oi atoms. Global heat transfer during crystal growth in a puller was simulated using STR Group's CGSim software package. A visual distribution of V and I concentrations inside a growing doped and thermally stressed Si ingot is very useful for improving the quality of large-diameter CZ-Si crystals.