Limited research has focused on the effect of high temperatures on the textile-reinforced mortar (TRM)-to-masonry bond. In this study, masonry prisms that were furnished with double-layered TRM strips were tested under shear bond conditions after their exposure to 200 °C and 400 °C for 1 h using the single-lap/single-prism setup. A total of four TRM systems were applied sharing the same type of textile –a dry AR glass fiber one– and different matrices: two cementitious matrices, namely a normal-weight (TRCNM) and a lightweight (TRCLM) one, and two counterpart alkali-activated matrices (TRAANM and TRAALM) based on metakaolin and fly ash. Specimens’ exposure to elevated temperatures did not alter their failure mode which was due to the sleeve fibers’ rupture along with core fibers’ slippage from the mortar. The residual bond capacity of the TRM systems decreases almost linearly with increasing exposure temperature. The alkali-activated textile reinforced mortars outperformed their cement-based counterparts in terms of bond strength at every temperature. All systems retained close to 50% of their original shear bond strength after heating at 400 °C. Per the type of binder, lightweight matrices resulted in either comparable (cement-based systems) or better (alkali-activated systems) heat protection at the TRM/masonry interface.
1 October 2023 in Journal of Composites for Construction
Reliable test methods that provide reproducible results are essential for the mechanical characterisation and standardisation of textile reinforced concrete (TRC). This paper presents the results of an interlaboratory study comprising uniaxial tensile tests and bond tests on TRC with various textile configurations. All laboratories conducted the experiments in accordance with predefined test protocols. The results were statistically evaluated with respect to scatter, repeatability, reproducibility and intraclass correlation coefficients (ICC). The uniaxial tensile test exhibited low interlaboratory scatter and a uniform mechanical response across all participants. Both the qualitative behaviour and the derived characteristic values showed close agreement, indicating that the applied procedure enables reproducible characterisation under controlled conditions. In contrast, the bond test revealed a higher level of scatter. This increased variability is attributed primarily to the greater sensitivity of the test arrangement and the inherent complexity of the bond interaction, rather than to systematic laboratory-dependent influences. Despite the larger numerical variability, the overall response characteristics were consistent across laboratories, demonstrating that the governing bond mechanisms were captured in a comparable manner. The results underline the need to combine quantitative evaluation with qualitative assessment when interpreting bond test data, providing a basis for further refinement and potential standardisation of the applied test methods.
Reducing the embodied carbon of reinforced concrete (RC) structures requires consideration not only of material composition but also of structural efficiency and the potential to retain and strengthen existing members. This study combines experimental testing and environmental assessment to evaluate alternative low-carbon strategies for RC flexural members and subsequently examines when retrofit is environmentally preferable to demolition and optimised replacement. Five large-scale beams were designed for comparable flexural resistance and tested under three-point bending, representing conventional concrete, eco-concrete, geometry-optimised eco-concrete, ultra-high-performance concrete (UHPC), and textile-reinforced concrete (TRC) strengthening. Their structural performance was combined with a global warming potential (GWP) assessment based on equivalent load-bearing capacity. All tested solutions exceeded the target design resistance. Compared with the conventional reference beam, binder substitution reduced embodied carbon by 15.4%, geometry optimisation by 36.0%, and the UHPC solution by 41.7%, although the latter result was sensitive to the reinforcement emission factor. The TRC-strengthened beam attained the highest measured flexural resistance of the investigated configurations, reaching 414.6 kNm, while the strengthening materials had a cradle-to-gate GWP of 71.0 kg CO2-eq. A parametric study subsequently compared TRC strengthening with demolition and replacement for different existing reinforcement ratios and required capacity increases. Within the investigated design space, TRC strengthening remained environmentally preferable wherever it was structurally feasible, providing approximately 27–90% lower GWP than replacement. No environmental crossover between the two strategies was identified before the structural feasibility limit of the TRC system was reached. The results demonstrate that low-carbon structural decisions should be based on equivalent structural performance and that retaining and strengthening existing RC members can provide substantial carbon savings compared with reconstruction when the required capacity increase can be achieved through retrofit.