To improve the surface properties of austenitic stainless steels, a thick S-phase layer was prepared by using a novel critical temperature nitriding (CTN) process. The properties of the thick S-phase layer were optimized by controlling the process parameters. The microstructures and phase compositions of CTN-treated layers were characterized by the optical microscope, scanning electron microscope and X-ray diffraction, respectively. The surface properties, including corrosion and wear resistance, were systematically investigated by the electrochemical workstation, micro-hardness tester and ball-on-disk tribometer, respectively. The results showed that a thick S-phase layer with a thickness of 18 to 25 μm can be fabricated in a short time by critical temperature nitriding, which represented higher efficiency than conventional low-temperature nitriding. Although the most top surfaces of CTN-treated layers contain massive iron nitrides, there are no precipitates in the inner nitrided layer. The electronic work function calculated by first-principles method has confirmed that those iron nitrides had a slight influence on the corrosion resistance of nitrided layers. The optimized CTN-treated layer exhibited a comparable corrosion resistance and wear resistance as the low-temperature nitrided layer. The CTN process is considered a potentially highly efficient surface modification method for austenitic stainless steels.
In this study, low-pressure gas nitriding (gas pressure of 0.01 MPa) was conducted to produce a thicker nitrided layer with high hardness and anti-corrosive properties on AISI 304 austenitic stainless steel. The effects of nitriding temperature and duration on the microstructure and surface property of nitrided layers were systematically evaluated by using optical microscope, X-ray diffraction, elemental analysis, microhardness test and potentiodynamic polarization tests. The samples were also treated under conventional gas pressure of 0.1 MPa for comparison. The results show that the low-pressure gas nitriding could restrain the precipitation of chromium nitrides effectively, which is beneficial for obtaining a thicker nitrided layer. Although the activation energy of nitrogen diffusion for low-pressure nitriding (220 kJ mol−1) is higher than that for the atmospheric pressure nitriding (196 kJ mol−1), the thickness of nitrided layers for low pressure nitriding could reach to a comparable value as that for the conventional atmospheric pressure nitriding. More importantly, the surface toughness and corrosion resistance of nitrided layers could be improved by low-pressure nitriding, which is mainly attributed to the optimized nitrogen content in nitrided layers and the reduced precipitation of chromium nitrides under low-pressure.
19 September 2019 in Journal of Failure Analysis and Prevention