Background: Composite material is being used in vehicles for protective structures against blast loading. Limited data is available which compare experimental works and numerical analysis in the open field environment. More data is needed in this area in order to be able to predict and use composite materials safely.Methods: In this work, the response of woven glass/epoxy composite plates under blast loading was investigated, both experimentally and numerically. The plate was manufactured using glass/epoxy woven Cytec 120 °C curing system. The explosive material was Tri-Nitro-Toluen (TNT) with different masses, which are 60, 80, and 100 g. The stand-off distance was also varied, ranging from 300 up to 1000 mm. In the experimental work, a sewing needle pin was put under the plate to record the maximum deformation of the plate during TNT explosion. In the numerical analysis, LS-DYNA was used extensively. The composite plate was modeled as shell elements using MAT54, and the failure criteria was Chang-Chang failure criteria. The explosive TNT material was modeled in two different ways. First, it was modeled using CONWEP and the second was modeled using Smooth Particle Hydrodynamics (SPH). The numerical analysis results were then compared with the experimental data for the case of maximum deformation.Results: Experimentally, the sewing needle method was able to measure the plate maximum deformation during the explosion. The numerical analysis showed that the SPH model gave better agreement with experimental results compared with CONWEP method. The SPH results were in the range of 8–18% compared to experimental data, while the CONWEP results were in the range of 14–43%.Conclusion: Albeit its simplicity, sewing needle method was able to measure the maximum deformation for blast loading experimentation. The SPH model was better compared with CONWEP method in analyzing the response of composite plate subjected to blast loading.
16 May 2024 in International Journal of Aerospace Engineering
This paper presents research on the use of anisogrid lattice structures in fighter wing applications. While the anisogrid lattice structure has been widely used in spacecraft structures, its implementation in main aircraft structures is still limited. The study is aimed at investigating the feasibility of utilizing an anisogrid lattice structure in fighter wing design. The analysis and optimization focus on determining the optimal weight of the composite wing structure, considering static, buckling, and flutter failure constraints. Various lift distributions, including triangular, Schrenk, and constant, are applied to evaluate the structures response to static failure caused by aerodynamic loads. The anisogrid structure design incorporates inclined lattice elements between ribs and spars, with spar arrangement in the wing box featuring an anisogrid configuration. The anisogrid lattice structure is expected to produce higher bending and torsional stiffness compared to conventional orthogonal structures, producing better flutter and buckling characteristics. The optimized wing structure successfully meets static, buckling, and flutter load requirements at speeds below 500m/s. The study showcases triangular, Schrenk, and constant load distributions resulting in half-wing masses of 504, 571, and 707kg, respectively. The results show that flutter and buckling loads are no longer the critical loads in wing structural design but static load.
Due to their anisotropic behavior, composite structures are weak in transverse direction loading. produces transverse cracks, which for a laminated composite, may lead to delamination and total failure. The transition from transverse crack to delamination failure is important and the subject of recent studies. In this paper, a simulation of transverse crack and its transition to delamination on cross-ply laminate was studied extensively using a cohesive element Finite Element Method (FEM). A pre-cracked [0/90] composite laminate made of bamboo was modeled using ABAQUS/CAE. The specimen was in a three-point bending configuration. Cohesive elements were inserted in the middle of the 90° layer and in the interface between the 0° and 90° layer to simulate transverse crack propagation and its transition to delamination. A load–displacement graph was extracted from the simulation and analyzed. As the loading was given to the specimen, stress occurred in the laminates, concentrating near the pre-cracked region. When the stress reached the tensile transverse strength of the bamboo, transverse crack propagation initiated, indicated by the failure of transverse cohesive elements. The crack then propagated towards the interface of the [0/90] laminates. Soon after the crack reached the interface, delamination propagated along the interface, represented by the failure of the longitudinal cohesive elements. The result of the numerical study in the form of load–displacement graph shows a consistent pattern compared with the data found in the literature. The graph showed a linear path as the load increased and the crack propagated until a point where there was a load-drop in the graph, which showed that the crack was unstable and propagated quickly before it turned into delamination between the 0o and 90° plies.