Ti-6Al-4V with its eclectic array of excellent properties along with the combination of meticulous precision and flexibility offered by the laser powder bed fusion (LPBF) technology makes it a strong proponent in the field of engineering applications. As a substantial amount of research has paved the way to fabricate Ti-6AL-4V more effectively and efficiently, researchers are becoming more adventurous in finding out the optimal techniques to get better yields in terms of mechanical responses. This includes post-processing techniques i.e., heat treatment (HT) or introducing various alloying elements. Nevertheless, these techniques not only make the overall fabrication more expensive and time-consuming but also contradict the simplistic notion of additive manufacturing (AM) by imparting multistage fabrication without a considerable improvement overall. Here, we propose an innovative breakthrough in the field of Ti-6AL-4V fabrication with LPBF by introducing an in-situ approach to tackle the handicap mentioned in contemporary studies. By imparting multiple laser scans prior to and after the melting scan at each layer, a remarkable 37% improvement in yield strength (YS) can be achieved with higher elongation, while also maintaining a high relative density of around 99.99%.
An innovative in situ thermal approach in the domain of LPBF for Ti-6Al-4V fabrication has been carried out with results directing towards an improved fatigue life without the need for post-processing. The thermal process involves an additional laser scan with different process parameters to preheat the selected regions of each layer of the powder bed prior to their full melting. This preheating step influences the cooling rate, which in turn affects surface characteristics and subsurface microstructure, both of which are directly correlated with fatigue properties. A thorough analysis has been conducted by comparing the preheated samples with reference samples with no preheating. Without any additional thermal processing, the preheated samples showed a significant improvement over their reference counterparts. The optimized preheated sample showed an improved prior β-grain distribution with a circular morphology and thicker α laths within the even finer prior β-grain boundaries. Also, an overall increment of the c/a ratio of the HCP α has been observed, which yielded lattice strain relaxation in the localized grain structure. Furthermore, a less-profound surface roughness was observed in the preheated sample. The obtained microstructure with all these factors delivered a 10% improvement in its fatigue life with better mechanical strength overall.
19 December 2024 in The International Journal of Advanced Manufacturing Technology
Significant attention has been directed to the need for a strong and lightweight welding technology for joining the NiTi shape memory alloys (SMAs) to stainless steel (SS). Dissimilar NiTi/SS joints suffer from the brittle and inevitable intermetallic components (IMCs) like TiFe, TiFe2 and FeNi that are formed during the welding process. To tackle this challenge, this study explores the use of an engineered magnetic field during the dissimilar laser welding of NiTi to SS. The presence of a magnetic field delivered a remarkable improvement in tensile strength (over 452 MPa) of the joint with a notable difference in microstructure. The effect of the magnetic field on microstructure was investigated; material characterizations showed brittle IMC-free microstructure and a change in grain growth mechanism from columnar to cellular growth during the solidification. Further, fractography analysis proved a ductile failure mode at the joint.