Objective: To test the hypothesis that adhesive remnant index (ARI) scores show no differences when examined under different magnifications. Materials and Methods: The study included 80 upper human premolars. Stainless steel brackets were bonded to the specimens with Transbond XT light cure adhesive and Transbond Plus Self Etch Primer (3M Unitek, Monrovia, Calif, USA). The brackets were debonded 24 hours after bonding with a universal testing machine (LLOYD Instruments, Segensworth, Fareham, England) at a cross head speed of 2.00 mm/min. The adhesive remnant was evaluated after debonding with the naked eye and under 10× and 20× magnification (Mag) using the 4-point scale described by Årtun and Bergland. Results: ARI scores were significantly different at different magnifications (P = .018). Scores were not significantly different when evaluated with the naked eye and under 10× Mag (P = .102). Scores were significantly different under 20× Mag and with the naked eye (P = .014); under 20× Mag, score 0 decreased from 12 to 6 and score 2 increased from 14 to 20 and also under 20× Mag and under 10× Mag (P = .046); the under 20× Mag score 1 decreased from 40 to 38 and score 3 increased from 14 to 16. Conclusion: ARI scores were significantly different under 20× Mag, where score 0 decreased and score 2 increased compared with the naked eye, while score 1 decreased and score 3 increased compared with 10× Mag.
Introduction: Biomimetic hydroxyapatite-based toothpastes have been investigated in recent years for their remineralizing activity on dental surfaces. The aim of the present study was to evaluate the efficacy of toothpaste containing biomimetic hydroxyapatite versus a 1450 pppm fluoride one in promoting the remineralization and desensitization of white spot lesions. Methods: 40 patients were randomly assigned to two different domiciliary oral hygiene treatments: toothpaste containing 1450 ppm of fluoride (control group) and toothpaste containing biomimetic hydroxyapatite (experimental group). Dental sensitivity/pain and dental erosion were assessed at baseline and after 15, 30, and 90 days using the following indexes: Schiff Air Index (SAI), Visual Analogue Scale (VAS), and Basic Erosive Wear Examination (BEWE). Results: Data were submitted for statistical analysis. SAI significantly decreased after 3 months (T3) of treatment only in the Trial group (p < 0.05). VAS values significantly decreased at T2 in the trial group (p < 0.05) with a further significant reduction at T3 (p < 0.05). BEWE scores did not significantly vary during the follow up neither in the trial nor in the control group. Conclusions: The hydroxyapatite-based toothpaste tested caused a reduction of hypersensitivity/pain values higher than conventional fluoride toothpaste.
In the last years, both medicine and dentistry have come across a revolution represented by the introduction of more and more digital technologies for both diagnostic and therapeutic purposes. Additive manufacturing is a relatively new technology consisting of a computer-aided design and computer-aided manufacturing (CAD/CAM) workflow, which allows the substitution of many materials with digital data. This process requires three fundamental steps represented by the digitalization of an item through a scanner, the editing of the data acquired using a software, and the manufacturing technology to transform the digital data into a final product, respectively. This narrative review aims to discuss the recent introduction in dentistry of the abovementioned digital workflow. The main advantages and disadvantages of the process will be discussed, along with a brief description of the possible applications on orthodontics.
Objective: To compare rebonding of orthodontic brackets based on the hypothesis that no difference would be found between the adhesive systems with respect to shear bond strength, mode of failure, and clinical failure rates. Materials and Methods: The three adhesive systems included two self-etch primers (Transbond and M-Bond) and a conventional phosphoric acid etch (Rely-a-Bond). The sample size was 20 premolars for each adhesive system. The shear bond strength was tested 24 hours after bracket bonding with the bonding/debonding procedures repeated two times after the first debonding. Bond strength, adhesive remnant index (ARI), and failure sites were evaluated for each debonding. Statistical analysis consisted of a two-way analysis of variance (ANOVA) followed by Scheffè analysis. The clinical portion evaluated 15 patients over a 12-month period. Results: The mean shear bond strengths after the first, second, and third debondings for Rely-a-Bond were 8.4 ± 1.8, 10.3 ± 2.4, and 14.1 ± 3.3 MPa, respectively; for Transbond 11.1 ± 4.6, 13.6 ± 4.5, and 12.9 ± 4.4 MPa, respectively; and for M-Bond 8.7 ± 2.7, 10.4 ± 2.4, and 12.4 ± 3.4 MPa, respectively. After the three debondings the mean shear bond strength increased significantly from the first to the third debonding for Rely-a-Bond and M-bond (P ≤ .001), but did not change for Transbond (P = .199). Conclusions: The original hypothesis is not rejected. The two self-etching primers showing higher or comparable bond strength to the conventional phosphoric etch with less adhesive remnant on the enamel surface after the first debonding. With repeated bonding/debonding, the differences in the bond strength, ARI, and failure site were not significantly different. There was no difference in the clinical performance of the three adhesive systems (P = .667).
1
17 September 2020 in American Journal of Orthodontics and Dentofacial Orthopedics