In this paper, nano-TiO2lubricating fluid was chosen as an advanced rolling lubricant to investigate its effect on the hot rolled surface and metallographic structure of SS41 steel strips. The tribological performances of nano-TiO2 lubricating fluid were measured by a four-ball tribotester. The hot rolling experiments under different lubrication conditions were carried out by a four-high rolling mill. The surface morphology, oxide scales and metallographic structure after hot rolling were observed using a confocal laser scanning microscope and scanning electron microscope (SEM), respectively. The composition of surface attachments was analyzed with X-ray photoelectron spectroscopy (XPS). The results indicate that the nano-TiO2 lubricating fluid has a better tribological performance. The surface defects on the hot rolled surface could be decreased. The phase composition of the surface still appears as a mixture of ferrite and pearlite. The surface of steel strips is not micro-alloyed with titanium as predicted. Additionally, the grain size of rolled steel strips which were lubricated with the nano-TiO2lubricating fluid decreased by nearly 50%, compared with traditional lubricating fluid. Furthermore, it was found that the thickness of the oxide layers on the surface reduced, whilst the Rockwell hardness of the oxide layers was enhanced as nano-TiO2 lubricating fluid was applied.
In this paper, triethanolamine modified graphene oxide (TMGO) has been synthesized by filtering and drying the high-temperature reaction solution of graphene oxide (GO) and triethanolamine. The tribological performance of TMGO and GO in de-ionized water were investigated using a four-ball tribometer. The microscopic morphology of the worn surface was analyzed by optical microscope and scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS). The results showed that the average friction coefficient (AFC) and wear scar diameter (WSD) of 0.1 wt % TMGO decreased by 21.9% and 6.2% compared with the two values of 0.1 wt % GO, and no corrosion occurred on metal surface. The minimum of the AFC and WSD occurred at 0.3 wt % TMGO. This study provides a new reference for the application of graphene oxide in lubrication.