In this work, 1060 pure aluminum was subjected to high rotating speed submerged friction stir processing (HRS-SFSP). The heat cycle curve of the processing area was measured by K-type thermocouple and temperature recorder. The microstructure, grain size, texture, and tensile fracture of the processing area were analyzed by electron backscattered diffraction and scanning electron microscopy. The results show that the HRS-SFSP caused severe plastic deformation of 1060 aluminum and produced fine recrystallized grains. The minimum average grain size was 0.686 μm at the 2-pass. In addition, the dislocation density in the stirred region was greatly reduced and the high angle grain boundaries (HAGBs) were dominant. The texture strength of pure aluminum increased with the increase in processing passes. The maximum hardness of 66.3 HV and ultimate tensile strength of 95.2 MPa were obtained at 1-pass, which were 86% and 33.9% higher than those of the base material, respectively. The hardness and strength of the stirring zone (SZ) decreased with the increase in the number of processing passes. Therefore, HRS-SFSP pure aluminum can obtain high strength and hardness while maintaining good plasticity.
High-strength aluminium alloys are prone to porosity and cracking during laser-based powder bed fusion of metals (PBF-LB/M) due to the complex solidification behaviour, thus limiting the preparation of high-quality aluminium alloys. In order to effectively reduce the defect formation, this study investigated the influence mechanism of different process parameters on the formation of porosity and cracks in Al-Zn-Mg-Cu alloys in the PBF-LB/M process by combining experimental and numerical simulation. The degree of influence of the process parameters on the temperature field and the temperature field on the defect formation was also quantified using path analysis. The results show that modulation of the process parameters can effectively reduce the formation of cracks and pores, although it is difficult to eliminate them. The melt pool temperature has a significant effect on the formation of porosity, and the temperature gradient has a significant effect on the formation of cracks. The degree of influence of laser power on the melt pool temperature and temperature gradient was greater than that of scanning speed, with values of 0.980 and 0.989, respectively. Therefore, the priority of modulating the laser power is higher than that of scanning speed in order to reduce the formation of defects more effectively.