Yin Yi

Dr. Yin Yi


Research Focus & Metrics

Academic Career Length

3Years (2024-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
24 July 2024 in Materials
Verified
Journal Article
Open access
PDF file
YYYin Yi
Yin Yi
WTWang Tiejun
Wang Tiejun
SQSigui Qin
Sigui Qin
WWWanjing Wang
Wanjing Wang
YSYingli Shi
Yingli Shi
HYHongxin Yu
Hongxin Yu
W-(0, 0.1, 0.3, 0.5) wt.% Hf (mass fraction, wt.%) materials were fabricated by the powder metallurgy method and hot rolling. The microstructure, mechanical properties, and high-temperature stability of alloys with varying compositions were systematically studied. The active element Hf can react with the impurity O segregated at the grain boundary to form fine dispersed HfO2 particles, refining the grains and purifies and strengthening the grain boundary. The average size of the sub-grains in the W-0.3 wt.% Hf alloy is 4.32 μm, and the number density of the in situ-formed second phase is 6.4 × 1017 m−3. The W-0.3 wt.% Hf alloy has excellent mechanical properties in all compositions of alloys. The ultimate tensile strength (UTS) is 1048 ± 17.02 MPa at 100 °C, the ductile fracture occurs at 150 °C, and the total elongation (TE) is 5.91 ± 0.41%. The UTS of the tensile test at 500 °C is 614 ± 7.55 MPa, and the elongation is as high as 43.77 ± 1.54%. However, more Hf addition will increase the size of the second-phase particles and reduce the number density of the second-phase particles, resulting in a decrease in the mechanical properties of the tungsten alloy. The isochronal annealing test shows that the recrystallization temperature of W-Hf alloy is 1400 °C, which is 200 °C higher than rolling pure tungsten.