Defects usually behave as imperfections in materials that significantly degrade their performance. However, the unusual optoelectronic performance in metal halide perovskites in the presence of defects opens the way for strain and optoelectronic properties tailoring with ion irradiation. Defects and strain engineering is performed in triple‐cation mixed halide perovskites using proton irradiation at 1 MeV and different fluences. At intermediate fluence, the initial polycrystalline film compressive strain (−0.15%) can be released, improving exciton lifetimes from about 500 ns to ≈1 µs. In contrast, high irradiation fluence is shown to restore compressive strain leading to sample degradation, with lower lifetime values (≈200 ns). Also, the phase segregation occurring under light illumination between bromine‐rich and iodine‐rich regions is shown to be defects‐mediated as the segregation rate increases by a factor of four for high proton irradiation fluence. The irradiation defects are revealed with low‐temperature photoluminescence (PL) through bound exciton radiative recombination mechanisms. The PL temperature dependence gives some insight into electron–phonon coupling mechanism and their modification with ion irradiation.
Luminescent carbon dots (CDs) were locally synthesized in the core of CYTOP fibers using IR femtosecond laser direct writing (FLDW), a one-step simple method serving as a post-treatment of the pristine fiber. This approach enables the creation of several types of modifications such as ellipsoid voids. The CDs and photoluminescence (PL) distribute at the periphery of the voids. The PL spectral properties were studied through the excitation/emission matrix in the visible range and excitation/emission spectra in the UV/visible range. Our findings reveal the presence of at least three distinct luminescent species, facilitating a broad excitation range extending from UV to green, and light emission spanning from blue to red. The average laser power and dose influence the quantity and ratio of these luminescent CD species. Additionally, we measured the spatially resolved lifetime of the luminescence during and after the irradiation. We found longer lifetimes at the periphery of the laser-induced modified regions and shorter ones closer to the center, with a dominant lifetime ~2 ns. Notably, unlike many other luminophores, these laser-induced CDs are insensitive to oxygen, enhancing their potential for display or data storage applications.
8 January 2026 in Physical Chemistry Chemical Physics
We demonstrate a strategy for multi-level photoluminescence encryption–decryption, based on fs-laser-induced photoluminescence and enabled by rewritable excitation anisotropy introduced via polarized post-exposure in transparent organic substrates.