Carbon fiber reinforced plastic (CFRP) laminates are used as main structural members in many applications. Transverse cracks that form in 90° layers of CFRP laminates are mostly initial damage in the case where tensile loading is vertically applied to the 90° layers of CFRP laminates, and they are the origin of more serious damage of delamination and fiber breakage. It is thus important to predict quantitatively the transverse crack initiation of CFRP laminates subjected to cyclic loading to ensure the long-term reliability of the laminates. The initiation and multiplication behaviors of transverse cracks strongly depend on the laminate configuration, thickness, and thermal residual stress. Therefore, a model based on the Walker model was proposed to predict transverse crack initiation in CFRP cross-ply and quasi-isotropic laminates under cyclic loading in the present study. The usefulness of the proposed model was verified with 10 different CFRP laminates formed from four different prepregs with epoxy resin matrices. The analysis results were in good agreement with experimental results. The fatigue life was expressed with three constants, which related to the fatigue strength reduction, the normalized fatigue strength at N = 1 cycle, and the contribution of stress amplitude to the fatigue life, and they are independent of the laminate configuration.
The damage process of composite materials, such as short fiber-reinforced plastics (SFRP), is complex. Therefore, it is necessary to accurately represent the damage process in fatigue life prediction. Herein, fatigue life prediction was conducted by combining the digital image correlation method, which is a non-destructive testing technique, with a convolutional neural network (CNN), using Xception as the network architecture. High prediction accuracy was obtained when training and testing were performed on the same SFRP specimens. In contrast, using different specimens for training and testing resulted in lower accuracy. This issue may be improved by increasing the number of specimens. The regions of interest in the model were visualized by Gradient-weighted Class Activation Mapping. Notably, the model indicated the breaking point as the region of interest from the early stages of the test. The breaking point was identified at an earlier stage by the CNN than by visual inspection, demonstrating the potential for a new method of damage observation.
5 June 2022 in Fatigue & Fracture of Engineering Materials & Structures
This study is aimed at clarifying the mechanism of effectively healing fatigue cracks in steel; austenitic stainless steel, SUS304; and hot work tool steel, SKD61, using high‐density pulsed current. The results show that the current concentration occurred at the crack tip for SUS304, and crack closure was observed near the fatigue crack tip. On the other hand, crack closure was observed at the notch tip in SKD61. The fatigue crack closure phenomena were verified by finite element analysis, revealing that contact pressure was applied behind the crack tip owing to local bending deformation associated with residual stress near the crack tip. For effective crack healing, it is necessary to bond the interface leveraging compressive stress and Joule heat generated at the crack tip during current application.
With the recent demand for weight reduction, structural materials for transportation equipment are being replaced by carbon-fiber-reinforced thermoplastics (CFRTPs). Therefore, techniques to join CFRTPs to alloys are needed. In this study, the fatigue delamination growth of bonded CFRTP/aluminum alloy joints was characterized. The specimens were bonded in three ways, using adhesive, direct chemical bonding, and direct chemical bonding with a nanostructured surface. The type of the specimen was double cantilever beam (DCB) specimen, which consisted of aluminum alloy (A5052) and plain woven CFRTP. The lay-up of the CFRTP was [(0,90)] 9 and the used matrix was PA6. Fatigue loading was applied in displacement control mode. The ratio between the minimum and maximum displacement was 0.1, and the test frequency was 5 Hz. The crack length during the fatigue tests was obtained by compliance calibration. Fatigue was characterized by constructing a Paris diagram for each specimen type. The fracture surface distinctively changed from smooth brittle-like fracture to hair-like ductile fracture post fabricating a nanostructure and chemical bonding. As a result, the fatigue crack growth resistance of the specimen with the nanostructure significantly improved due to the hair-like ductile fracture.