Overhead transmission line is the main method of power transmission. Conductors, insulators, and towers are the primary electrical equipment of overhead transmission lines. Due to overhead transmission lines work in the natural environment, problems such as icing, corona discharge, contamination deposition, and corrosion will arise. As a result, some accidents may occur, which cause enormous economic losses. The above problems can be solved by coating functional coatings with superhydrophobic, semiconductive, anti-corrosion, and other characteristics on electrical equipment, which has the advantages of low cost and high efficiency. Therefore, functional coatings have become a research hotspot in the field of external insulation in recent years. In view of the various problems of different electrical equipment in overhead transmission lines, distinctive solutions need to be adopted, so this review classifies the coatings according to the usage scenarios and functions. In each category, first briefly outlines the causes of the electrical equipment problem, then introduces the mechanism of using this type of functional coating to solve the problem, next summarizes the development and application status of this type of coating, after summarizes the limitations of this coating, and finally provides a summary of the key issues in the research of functional coatings and gives an outlook on potential future research directions. This review intends to provide readers with a comprehensive overview of the performance principles and current application status of functional coatings for overhead transmission lines.
Composite insulators have been extensively adopted in electric transmission lines due to their preferable resistance to contamination flashover. To generally ensure the function of power networks, it is of crucial importance to perform regular online detection and the timely renewal of poor-quality insulators. As the most extensively employed method for the online analysis of composite insulators, infrared (IR) detection is defective based on the false detection rate and the high rate of undetected inner defects. Via numerical simulation and analysis and a test of the simulation model, this paper seeks to systematically ascertain how the defect temperature and IR results are related to each other for different types of conditional thermal defects in composite insulators, especially the relationship between humidity and heating. Finally, considering our previous findings and the on-site feasibility of the methods, some suggestions for IR detection methods regarding composite insulators are proposed. The findings of this paper are conducive to elucidating the conduction of heat flow through the composite insulators and reducing the false detection rate arising from moisture and inner defects. Furthermore, the optimized IR detection method targeting high humidity areas can also be valuable in reference to other power supply units.
16 June 2022 in IEEE Transactions on Dielectrics and Electrical Insulation
The intrusion of moisture may induce an abnormal increase in temperature or may even cause fractures in insulation equipment. Therefore, the hygroscopicity of rubber materials must be characterized. However, the existing methods for weighing organic polymer materials, such as silicone rubber, for moisture-absorption tests are time-consuming. In this article, a practical method for testing the moisture-absorption performance of silicone rubber materials for external insulation is proposed. The basic characteristics of the Langmuir diffusion equation for the water-absorption characteristics of silicone rubber are analyzed. A Langmuir curve fitting method based on the contraction–expansion (C–E) algorithm is developed, and its fitting effect is preliminarily verified by combining the experimental errors obtained from the experiment. Results show that the fitting effect has a strong relationship with the initial range of diffusion coefficient, bonding coefficient, and debonding coefficient. The time-consuming process of directly applying the fitting method is reduced from 70 to 50 days. The initial ranges of diffusion, bonding coefficient, and debonding coefficient are determined via the results of molecular simulations and experiments combined with an analysis of the literature. A prediction model is optimized and then validated against the experimental data from the recent literature on the water-absorption characteristics of silicone rubber at different temperatures. The experimental time required to reach saturated water absorption is remarkably reduced from 70 days to 1 day. Therefore, the method developed herein is feasible for engineering applications. Moreover, the entire water-absorption curve can be possibly plotted with an error of not greater than 5% via this prediction method.
It is crucial to ensure the adhesive quality of the interface in composite insulation equipment for power grid security. Due to viscoelasticity of silicone rubber and roughness of interface, the thickness of the local air layer in the defective interface is <100 μm. This kind of defect is called micro‐debonding defect in this paper, and it is significantly smaller than the millimetre‐scale air gaps which could be defected by the x‐ray, THz, and traditional ultrasonic method. It remains challenging to detect the micro‐debonding in composite insulation by non‐destructive testing methods. In this paper, the acoustic model and bi‐linear stiffness model for micro‐debonding in different stages are established. Accordingly, a conjecture is proposed that the bonding property of composite insulation is related to the acoustic impedance of interface and non‐linear distortion of its constitutive relation. The result obtained from numerical simulation with and without defect is compared with the high‐power ultrasonic experimental data to validate the correctness of the theoretical model. In addition, it can be concluded that the non‐linear distortion of high‐power ultrasonic wave can be effectively used to diagnose micro‐debonding defect at the interface of composite insulation in its early stage (1–20 μm).