Replacing ordinary Portland cement-based materials with alkali-activated industrial wastes is often limited because of significant volume changes occurring in these materials at early age. This experimental study aims to quantify the extent of the volume changes and explore the underlying mechanisms of pastes composed of slag and fly ash (ratio 50:50) which are activated by sodium hydroxide and sodium silicate. Eight compositions were tested, with silica modulus (Ms) varying between 1.04 and 1.58 and with solution-to-binder ratios (S/B) varying between 0.47 and 0.70. Specimen length changes in sealed conditions are monitored by applying repeated thermal variations in an adapted AutoShrink device and are accompanied by isothermal calorimetry, uniaxial compressive strength, and internal relative humidity (IRH) tests. This way, the temporal evolutions of autogenous strains, the coefficient of thermal expansion (CTE), the heat release, the apparent activation energy (Ea), the IRH and the strength are determined and compared to each other. Both the measured autogenous shrinkage and CTEs are rather large; they amount to 4,000–5,000 μm/m and roughly 40 μm/m/°C, respectively, at material ages of 2 weeks. An increase in S/B leads to a decrease in autogenous shrinkage and an increase in CTE. An increase in the Ms causes a decrease in both the autogenous shrinkage and the CTE. Most strikingly, autogenous shrinkage evolves linearly with the cumulative heat released by the binders. The IRH remains continuously above 94% during the first 2 weeks. The apparent activation energy amounts to roughly 74 kJ/mol and is virtually unaffected by S/B and Ms.
This research investigates the impact of solution concentration and solution-to-binder ratio (S/B) on the volume changes in alkali-activated slags with sodium hydroxide at 20 °C. Autogenous and thermal strains are monitored with a customized testing device in which thermal variations are controlled. Consequently, both the autogenous strain and coefficient of thermal expansion (CTE) are determined. Heat flow and internal relative humidity (IRH) are also monitored in parallel, making this research a multifaceted study. The magnitudes of autogenous strain and CTE are higher than those of ordinary Portland cement paste. Decreasing the solution concentration or S/B generally decreases the autogenous strain (swelling and shrinkage) and the CTE. The shrinkage amounted to 87 to 1981 µm/m, while the swelling reached between 27 and 295 µm/m and was only present in half of the compositions. The amplitude of the CTE, which increases up to 55 µm/m/°C for some compositions while the CTE of OPC remains between 20 and 25 µm/m/°C, can be explained by the high CTE of the solution in comparison with water. The IRH of paste cannot explain the autogenous strain’s development alone. Increasing S/B eliminates the self-desiccation-related decrease.
This research investigates whether metakaolin can be used as a partial substitution for slag to mitigate significant volume changes in alkali-activated slags. Its effect on compressive strength and workability (as well as on isothermal calorimetry, autogenous strain, and coefficient of thermal expansion (CTE)) were found to depend on both the type and concentration of the alkaline activator. When using 8 M and 10 M sodium hydroxide (NaOH), increasing the substitution rate increased the compressive strength. With sodium silicate (Na2SiO3), compressive strength decreased as the substitution increased. Isothermal calorimetry revealed metakaolin’s dilution effect at 10% substitution. With 8 M NaOH, a third reaction peak appeared, whose magnitude increased with the substitution rate, while the second peak decreased. The swelling was increased at 10% substitution, followed by constant shrinkage in case of NaOH-activation. Shrinkage was mitigated with Na2SiO3-activation. Higher substitutions with 8 M NaOH resulted in a significant increase in the shrinkage rate and CTE, occurring when the third reaction peak appeared. A 10% substitution delayed the CTE increase but resulted in higher later-age values (dilution effect). The 20% substitution led to a similar final CTE value at 300 h, while 30% substitution resulted in a decrease in CTE after the initial increase.
This study investigates the influence of curing temperature (explored at 10 °C, 20 °C, and 30 °C) on the volume changes of alkali-activated slag (AAS) pastes with the aim of expanding existing knowledge on alkali-activated materials (AAMs). The focus was on autogenous and thermal strains, internal relative humidity (IRH), heat flow and cumulative heat, setting times, and workability. The results indicate that increasing the curing temperature to 30 °C reduces autogenous shrinkage, likely due to changes in the elastic modulus and viscoelastic properties, while promoting swelling, especially for higher molarities. The coefficient of thermal expansion (CTE), related to thermal strains, is higher when the curing temperature is increased, but its development is delayed. The IRH is influenced more by the activating solution’s molarity than by curing temperature, although temperature does affect the initial IRH. The study also revealed that higher curing temperatures accelerate chemical reactions and reduce setting times. The initial workability was significantly affected by the solution-to-binder ratio, while higher temperatures decreased workability, especially at higher molarities. These findings contribute to the understanding of how curing temperature influences the durability of AAS pastes, offering insights into optimized construction practices under varying environmental conditions.