Low-temperature additive manufacturing of magnesium (Mg) alloy implants is considered a promising technique for biomedical applications due to Mg’s inherent biocompatibility and 3D printing’s capability for patient-specific design. This study explores the influence of powder volume content, size, and morphology on the mechanical properties and viscosity of polylactic acid (PLA) matrix composite filaments containing in-house-produced magnesium–calcium (Mg-Ca) particles, with a focus on their application towards low-temperature additive manufacturing. We investigated the effects of varying the Mg-Ca particle content in a PLA matrix, revealing a direct correlation between volume content and bending strength. Particle size analysis demonstrated that smaller particles (D50: 57 μm) achieved a bending strength of 63.7 MPa, whereas larger particles (D50: 105 μm) exhibited 49.6 MPa at 20 vol.%. Morphologically, the filament containing spherical particles at 20 vol.% showed a bending strength that was 11.5 MPa higher than that of the filament with irregular particles. These findings highlight the critical role of particle content, size, and shape in determining the mechanical and rheological properties of Mg-Ca/PLA composite filaments for use in material extrusion additive manufacturing.
Controlling electrochemical heterogeneity in powder-processed magnesium (Mg) alloys is important for biodegradable implant applications because oxide-bearing prior particle boundaries (PPBs) can influence corrosion behaviour. In this study, WE43 alloy powder compacts were sintered at 400-600 °C for 1-9 h to determine how post-processing affects phase evolution, yttrium (Y) redistribution, densification, and mechanical performance. X-ray diffraction (XRD), scanning electron microscopy with energy-dispersive spectroscopy (SEM/EDS), and CALPHAD analysis showed that the rapidly solidified Mg3Nd phase in gas-atomised powder dissolved during sintering. Mg24Y5 appeared under lower-temperature conditions, whereas increasing temperature and time promoted Mg41Nd5 formation and Y segregation to O-rich PPBs, producing Y2O3-indexed boundary phases. Arrhenius-Fick diffusion analysis supported a diffusion-controlled depletion of Y from the α-Mg matrix and enrichment at PPBs. Scanning Kelvin probe force microscopy (SKPFM) revealed that this segregation creates the highest Volta potential (ΔV) between the matrix and PPBs for samples sintered at 500 °C. However, the ΔV is relatively lower at 600 °C due to the intermetallic dissolution at the α-Mg matrix and rare-earth-rich liquid phase formation at the PPBs. Porosity decreased to a minimum of 1.0 vol.% at 500 °C for 9 h, while the highest ultimate compressive strength (271.8 MPa) was obtained at 600 °C for 1 h. Although 600 °C enabled rapid densification, prolonged holding did not improve mechanical performance. Therefore, to optimise mechanical performance without compromising corrosion resistance, understanding the phase evolution is the key factor.