A series of V2O5–WO3/TiO2 catalysts with different vanadium loading amounts were prepared by an impregnation method and were characterized by XRD, Raman spectroscopy, XPS, DRIFTS, Py-DRIFTS, NH3-TPD, H2-TPR, etc. The results show that the catalytic activity is related to the ratio of V4+/V5+. The variation of the V4+/V5+ ratio caused by the different dispersion states of vanadia oxide leads to changes in the surface acidity and redox properties of the catalysts. As the V4+/V5+ ratio reaches the maximum value, the apparent activation energy (Ea) required to form the transition state on the Brønsted acid sites is the lowest. Artificial regulation of vanadium loading to properly increase V4+/V5+ content may affect the interactions between V, W, O and Ti atoms, which enhances NH3-SCR reaction performance.
In this study, steerable nanosized TiO2 was prepared by a novel and facile cetyltrimethyl ammonium bromide (CTAB)-assisted hydrothermal process. Different from traditional hydrothermal methods, diverse amounts of CTAB and TiO2 nanopowders were added into a NaOH aqueous solution for hydrothermal reaction. The products were characterized by thermogravimetric differential scanning calorimetry (TG-DSC), X-ray diffraction (XRD), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), X-ray photoelectron spectroscopy (XPS) and N2 adsorption–desorption. The results show that adding 0.04 mol L−1 CTAB in the hydrothermal reaction contributes to the efficient preparation of TiO2 nanotubes. It is found that the length of TiO2 nanotubes can be tuned from 50 nm to several hundred nanometers by simply adjusting the CTAB concentration from 0.01 to 0.04 mol L−1. It is noteworthy that the as-prepared TiO2 consists of nanosheets with the further increased amount of CTAB to 0.2 mol L−1. Furthermore, the possible formation mechanism of nanosized TiO2 with controllable morphology obtained from the CTAB-assisted hydrothermal method was also proposed.
A series of Mn-Ce-V-WOx/TiO2 composite oxide catalysts with different molar ratios (active components/TiO2 = 0.1, 0.2, 0.3, 0.6) have been prepared by wet impregnation method and tested in selective catalytic reduction (SCR) of NO by NH3 in a wide temperature range. These catalysts were also characterized by X-ray diffraction (XRD), Transmission Electron Microscope (TEM), in situ Fourier Transform infrared spectroscopy (in situ FTIR), H2-Temperature programmed reduction (H2-TPR) and X-ray photoelectron spectroscopy (XPS). The results show the catalyst with a molar ratio of active components/TiO2 = 0.2 exhibits highest NO conversion value between 150 °C to 400 °C and good resistance to H2O and SO2 at 250 °C with a gas hourly space velocity (GHSV) value of 40,000 h−1. Different oxides are well dispersed and interact with each other. NH3 and NO are strongly adsorbed on the catalyst surface and the adsorption of the reactant gas leads to a redox cycle with the valence state change among the surface oxides. The adsorption of SO2 on Mn4+ and Ce4+ results in good H2O and SO2 resistance of the catalyst, but the effect of Mn and Ce are more than superior water and sulfur resistance. The diversity of valence states of the four active components and their high oxidation-reduction performance are the main reasons for the high NO conversion in this system.
1 September 2008 in Journal of Alloys and Compounds