This article presents a synthesis of recent studies focused on the corrosion product layers forming on carbon steel in natural seawater and the link between the composition of these layers and the corrosion mechanisms. Additional new experimental results are also presented to enlighten some important points. First, the composition and stratification of the layers produced by uniform corrosion are described. A focus is made on the mechanism of formation of the sulfate green rust because this compound is the first solid phase to precipitate from the dissolved species produced by the corrosion of the steel surface. Secondly, localized corrosion processes are discussed. In any case, they involve galvanic couplings between anodic and cathodic zones of the metal surface and are often associated with heterogeneous corrosion product layers. The variations of the composition of these layers with the anodic/cathodic character of the underlying metal surface, and in particular the changes in magnetite content, are thoroughly described and analyzed to enlighten the self-sustaining ability of the process. Finally, corrosion product layers formed on permanently immersed steel surfaces were exposed to air. Their drying and oxidation induced the formation of akaganeite, a common product of marine atmospheric corrosion that was, however, not detected on the steel surface after the permanent immersion period.
Iron palaeometallurgy was carried out on three artefacts, classified as nails and excavated from the archaeological site of Loiola (La Arboleda, Biscay, northern Spain), to investigate Roman manufacturing techniques. Energy Dispersive Spectroscopy (EDS) coupled with Environmental Scanning Electron Microscopy (ESEM) and micro-Raman spectroscopy were used to obtain elemental composition and structural characterization of mineral phases. Metallurgical properties and crystallographic texture were studied by combining microscopic methods such as optical microscopy (OM), Electron Backscatter Diffraction realized in environmental mode (EBSD) and measurements of local Vickers microhardness. The three artefacts had different microstructures, distinguished by a large gradient of carbon content, although important segregations (inclusions) were observed in all of them. Two pearlite-rich artefacts showed a high density of structural defects (geometrically necessary dislocations and large crystallographic orientation gradients in pearlitic ferrite, curved pearlitic cementite) resulting from a high level of plastic deformation that occurred during the manufacturing process. The third artefact consisted of pure ferrite without structural defects. This one was clearly manufactured differently from the two others, so it probably had another functionality.
In the archaeometallurgical study of iron nails to investigate Roman manufacturing processes, multi-analyte characterization provides information on alloy composition and microstructure. Nails from the Roman sites of Forua, Aloria, and Iuliobriga (northern Spain) were studied. To characterize the iron phases and microstructures of the nails, optical microscopy (OM), scanning electron microscopy coupled with electron-dispersive spectroscopy (SEM-EDX), micro-Raman spectroscopy, electron backscatter diffraction (EBSD) realized in environmental mode, and microhardness measurements were carried out. The chemical composition of the metal was determined by X-ray fluorescence (XRF). The corrosion mineralogical composition was determined by powder X-ray diffraction (XRD). Aggressive burial conditions had a significant effect on the forms of corrosion of the Forua nails to the point of complete iron loss. Examination of the metal of the nails from the Aloria site revealed that most of the ironwork was made in the villa’s own forge. In the case of the Iuliobriga nails, different degrees of forging were identified associated with different workshops.
The possible incorporation of Al and Zn issuing from galvanic anodes in the calcareous deposit forming on carbon steel surfaces subjected to cathodic protection was studied via three methodological approaches. The calcareous deposits were analyzed by X-ray diffraction for phase composition and X-ray fluorescence spectroscopy for chemical composition. First, a calcareous deposit formed on the steel pile of a seaport installation, sampled far (2 m) from the closest galvanic anode, was found to incorporate a small amount of the pollutants present in the seawater (Zn, Ti, Cu). An in situ experiment performed at another seaport focused on the calcareous deposit formed on steel surfaces close to the anode. In this case, a small amount of Zn directly issuing from the anode was incorporated in the deposit. This amount remained low as it corresponded to Zn(II) species adsorbed on the surface of aragonite crystals. Finally, laboratory experiments were performed with Zn(II) and/or Al(III) chlorides (10−3 mol L−1 each) added to seawater. With both Zn(II) and Al(III), a Zn(II)-Al(III) hydroxychloride precipitated in the bulk seawater. With only Al(III), and under a higher cathodic current density, Al(III) could be incorporated in a deposit mainly composed of brucite, but only in small amount.