Shuangkuai Dong

Shuangkuai Dong


Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
12 December 2022 in Applied Sciences
Verified
Journal Article
Open access
PDF file
YGYuanyuan Gong
Yuanyuan Gong
SDShuangkuai Dong
Shuangkuai Dong
LLLiuyan Liu
Liuyan Liu
Fufei WuFufei Wu
Fufei Wu
The phosphogypsum is a by-product of the phosphate fertilizer industry. It has accumulated over several decades, and not only takes up a large amount of land, but also poses a significant risk to the environment and resource waste. In order to promote the use of phosphogypsum, its hydration hardening characteristics are studied using a scanning electron microscope, X-ray diffractometer and mercury intrusion porosimeter. When the amount of phosphogypsum is increased, a decreasing trend in the reaction degree, non-evaporable water and portlandite is observed. Among them, the reaction degree and non-evaporable water, flexural strength and compressive strength reached their maximum when the content of phosphogypsum was 10%, which were as follows: 22.34 %, 21.13 %, 9.02 MPa and 49.8 MPa, respectively. Meanwhile, phosphogypsum can participate in the secondary hydration reaction in the system and act as a microaggregate. The addition of no more than 30% phosphogypsum can enhance mechanical characteristics, reduce porosity, refine pore size distributions and densify the microstructure. The findings of this study may aid in the production of phosphogypsum-based composite cementitious materials with superior performance, thereby promoting phosphogypsum recycling and protecting the environment.

4 February 2023 in Sustainability
Verified
Journal Article
Open access
PDF file
SDShuangkuai Dong
Shuangkuai Dong
QZQi Zhuo
Qi Zhuo
LCLiangliang Chen
Liangliang Chen
Fufei WuFufei Wu
Fufei Wu
LXLilan Xie
Lilan Xie
The combination of red mud (RM) and phosphogypsum (PG) can exert the alkalinity of RM and the acidity of PG as a calcium source to promote the gel hardening of composite cementitious material, which effectively improves the reutilization efficiency of RM and. In this study, the effects of the ratio and content of pretreated RM and PG on the non-evaporated water, porosity, hydration products, mechanical properties, pore size distribution, and microstructure of composite cementitious materials were investigated. The results show that, with the incorporation of PG, RM, PG, and RM, the non-evaporable water content, reaction degree, compressive strength, and flexural strength show a downward trend after rising first, and their values reach the maximum with 10% PG and 10% RM, which are higher than a pure cement system, while 70% PG, 70% RM, 70% RM + 10% PG, and 70% PG + 10% RM have the reverse effect. The results of hydration products, pore size distributions, and microstructure indicate that adding an appropriate dosage of RM and PG can efficaciously improve the compactness of cement systems. Nevertheless, the research results can contribute to using the combination of PG and RM to manufacture sustainable cementitious materials with good performance, and achieve the purpose of environmental protection and industrial solid waste resource recycling.

26 February 2023 in Buildings
Verified
Journal Article
Open access
PDF file
SDShuangkuai Dong
Shuangkuai Dong
SYSonghan Yu
Songhan Yu
LCLiangliang Chen
Liangliang Chen
QZQi Zhuo
Qi Zhuo
Fufei WuFufei Wu
Fufei Wu
LLLiuyan Liu
Liuyan Liu
Nano-metallic oxide particles have been found to be potentially effective microstructural reinforcements for cement mortar and have become a research hotspot in recent years for nano-modification technology of building materials. However, different conclusions have been obtained due to various researchers used different research methods, which have resulted in a deficiency for the performance comparison between different nano-metallic oxide particles. In the present study, the effects of five kinds of nano-metallic oxide particles, namely nano-MgO, nano-Al2O3, nano-ZrO2, nano-CuO, and nano-ZnO, on the performance of cement mortar at 28 days and 730 days in terms of mechanical, durability, microstructure, and pore size distribution properties by performing different experiments were investigated. Test results show that the dosage of nano-MgO, nano-Al2O3, nano-ZrO2, nano-CuO, and nano-ZnO is 2%, 1%, 1%, 1%, and 2%, respectively, where they can significantly prove the compressive and flexural strengths, decrease the porosity, drying shrinkage, and permeability, and refine the pore size distribution of cement mortar. It can be seen through SEM analysis that nano-metallic oxide particles can promote cement hydration, and also refine the size and distribution of Ca(OH)2 crystal, but the specific principles are different. The analysis concluded that the five kinds of nano-metallic oxide particles can play a filling role in cementitious materials to improve the denseness and surface activity role to promote the hydration of cement particles, thus improving the mechanical properties, durability, and pore size distribution of cementitious materials, with the order of their modification effect on cement-based materials being nano-ZrO2 > nano-MgO > nano-Al2O3 > nano-ZnO > nano-CuO.

15 March 2023 in Molecules
Verified
Journal Article
Open access
PDF file
SDShuangkuai Dong
Shuangkuai Dong
SYSonghan Yu
Songhan Yu
LCLiangliang Chen
Liangliang Chen
QZQi Zhuo
Qi Zhuo
Fufei WuFufei Wu
Fufei Wu
LLLiuyan Liu
Liuyan Liu
The main component of phosphogypsum (PG) is CaSO4·2H2O. PG contains a few impurities, heavy metals, and radioisotopes, which limit the use of PG and pose a danger to the environment. In this study, under the excitation of a sodium hydroxide solution, the rheological properties of a paste with granulated blast-furnace slag (GGBS) and PG treated with ultrasonic water washing were investigated. Experimental results showed that the ratio of GGBS to PG and the amount of sodium hydroxide solution significantly affect the density and viscosity of the paste, but the effect patterns of both are different. The maximum viscosity was 498 mPa·s when the ratio of GGBS to PG was 4:1. When the ratio changed from 3:2 to 1:4, the viscosity of the paste gradually decreased by 15.5%, 32.1%, 36.1%, and 46.8%, respectively. In contrast, the ratio of GGBS to PG had a greater effect on the viscosity than the amount of sodium hydroxide solution in terms of the standard consistency water consumption, viscosity, and water release ratio. The larger the PG ratio, the smaller the density, viscosity, and water release ratio of the paste. The variation in the ratio of GGBS to PG had a significant effect on the water film thickness of the paste, demonstrating that the larger the PG mixture, the larger the water film thickness of the paste, which reached 1.122 μm, 2.31 times the minimum water film thickness of the paste. At the same time, the water film thickness of the paste was negatively correlated with the water consumption of the standard consistency, viscosity, and water release ratio, and was positively correlated with the fluidity.

8 June 2024 in Buildings
Verified
Journal Article
Open access
PDF file
ZZZhenhua Zhao
Zhenhua Zhao
Fufei WuFufei Wu
Fufei Wu
SDShuangkuai Dong
Shuangkuai Dong
QZQiuyue Zhang
Qiuyue Zhang
CHChuanteng Huang
Chuanteng Huang
LCLiangliang Chen
Liangliang Chen
In present study, the effects of varying dosages of combined red mud on the microstructure and hydration process of low-carbon composite cementitious material. The findings indicated a gradual decrease in the reactivity of RM, following a linear trend. The non-evaporable water content of the composite binder exhibited an initial increase followed by a subsequent decrease, with the optimal content identified at 10%, for RM content ranging from 10% to 90%, non-evaporable water decreases linearly. Optimal bending strength and compressive strength were achieved in the mortar when incorporating 10% of RM, reaching 8.56 MPa and 51.2 MPa at 28 days, respectively. The porosity was at its lowest when the RM content was added at 10%, but further increasing RM dosage was reversed. The pore size distribution aligned with the experimental findings on porosity. X-ray diffraction (XRD) analysis revealed the involvement of RM in the secondary hydration reaction, thereby enhancing the mechanical properties of low-carbon composite cementitious material. The optimal content of RM is suggested to be 10%, with a maximum recommended limit of 30%. The analysis has shown that red mud particles serve a dual purpose in low-carbon composite cementitious material. They enhance compactness by acting as fillers and promote cement hydration through surface activity, thereby enhancing mechanical properties, durability, and pore size distribution.

7 August 2025 in Materials
Verified
Journal Article
Open access
PDF file
YCYang Cai
Yang Cai
QLQiumei Liu
Qiumei Liu
Fufei WuFufei Wu
Fufei Wu
SDShuangkuai Dong
Shuangkuai Dong
QZQiuyue Zhang
Qiuyue Zhang
XYXin Yang
Xin Yang
The resource utilization of construction waste and industrial solid waste is a crucial aspect in promoting global urbanization and sustainable development. This study focuses on the preparation of mine backfill materials using construction waste in combination with various industrial solid wastes—ground granulated blast furnace slag (GGBFS), fly ash (FA), silica fume (SF), phosphorus slag (PS), fly ash–phosphorus slag–phosphogypsum composite (FA-PS-PG), and fly ash–phosphorus slag–β-phosphogypsum composite (FA-PS-βPG)—under different substitution rates (50%, 55%, 60%) as control parameters. A total of 19 mix proportions were investigated, evaluating their slump, dry density, compressive strength, uniaxial compressive stress–strain relationship, micromorphology, and phase composition. The results indicate that, compared to backfill materials prepared with pure cement, the incorporation of industrial solid wastes improves the fluidity of the backfill materials. At 56 days, the constitutive model parameter a increased to varying degrees, while parameter b decreased, indicating enhanced ductility. The compressive strength was consistently higher with PS at all substitution rates. The FA-PS-PG mixture with a 50% substitution rate achieved the highest 56-day compressive strength of 8.02 MPa. These findings can facilitate the application of construction waste and industrial solid waste in mine backfilling projects, delivering economic, environmental, and resource-related benefits.