Vanadis 4E (V4E) is a powder metallurgical cold work tool steel predominantly used in application with demand for wear resistance, high hardness, and toughness. It is of interest to have a processing route that enables full density starting from clean gas-atomized powder allowing component shaping capabilities. This study presents a process involving freeze granulation of powder to facilitate compaction by means of cold isostatic pressing, followed by sintering to allow for capsule-free hot isostatic pressing (HIP) and subsequent heat treatments of fully densified specimens. The sintering stage has been studied in particular, and it is shown how sintering in pure nitrogen at 1150 °C results in predominantly closed porosity, while sintering at 1200 °C gives near full density. Microstructural investigation shows that vanadium-rich carbonitride (MX) is formed as a result of the nitrogen uptake during sintering, with coarser appearance for the higher temperature. Nearly complete densification, approximately 7.80 ± 0.01 g/cm3, was achieved after sintering at 1200 °C, and after sintering at 1150 °C, followed by capsule-free HIP, hardening, and tempering. Irrespective of processing once the MX is formed, the nitrogen is locked into this phase and the austenite is stabilised, which means any tempering tends to result in a mixture of austenite and tempered martensite, the former being predominate during the sequential tempering, whereas martensite formation during cooling from austenitization temperatures becomes limited.
When processing powder metallurgy (PM) steels, the conventional press and sinter route can reach a relative density up to 95%, which is insufficient for applications when dynamic mechanical performance is critical. In this study, a novel route is demonstrated consisting of cold isostatic pressing (CIP) followed by sintering and capsule-free hot isostatic pressing (HIP), allowing to achieve full density PM steels. Water-atomized steel powder admixed with 2 wt.% Ni was subjected to CIP and followed by sintering in 90N2/10H2 atmosphere at 1120 and 1250°C, and in vacuum (10−2 mbar) at 1250 and 1350°C, respectively. At the highest explored CIP pressure of 600 MPa, the three high-temperature sintering runs at 1250°C in 90N2/10H2 atmosphere and vacuum, and 1350°C in vacuum resulted in relative density of ∼94% and closed surface pores. This condition with necessary closed porosity then allowed subsequent capsule-free HIP after sintering, resulting in full densification of the components.