Geopolymer is a relatively new substance that has sparked a surge of research into nearly every field of geopolymers in recent years. It's still on the verge of becoming a competitive OPC concrete alternative. Mechanical, hardness, and fire resistance properties of geopolymer are exceptional. There has been no/limited research on the effect of fiber integration on fire resistance of geopolymer concrete. In fire-exposed concrete, fiber can help to resist spalling. The goal of this study is to develop materials that exhibit eco-friendly properties and better fire-resistant behavior. Moreover, the combined effect of binder materials and different fibers on the fire resistance of geopolymer concretes. According to the findings, the fire resistance of fiber-reinforced geopolymer concretes increased in the order of carbon fiber-based GPC, micro-steel fiber-based GPC, hooked steel fiber-based GPC, and polypropylene fiber-based GPC. Furthermore, as compared to slag and metakaolin-based GPC, fly ash-based GPC has greater stability and fire resistance. Fiber-reinforced GPC can also be used as a sustainable and durable building material in various construction applications where high performance is needed.
This study investigates fiber-reinforced cementitious composites (FRCCs), concentrating on the geometric features of soft micro- and macro-fibers with a lower elastic modulus and higher aspect ratios than steel fibers. There is no literature predicting the ratio of ultimate flexural strength to the initial cracking strength of FRCC. The composites were made using a cement-to-sand ratio of 1:2.5, with 20% fly ash as a partial substitution and two water-to-binder ratios (0.55 and 0.60). Carbon, polypropylene, and natural sisal fibers were added at quantities ranging from 0.4% to 2.27%, with aspect ratios ranging from 71 to 3750. Flexural strength was determined using 75 × 75 × 380 mm3 prisms, whereas compressive strength was evaluated using 50 mm cubes. Load–deflection curves were created to investigate fracture behavior. The post-cracking behavior was determined using the matrix compressive strength, fiber type, amount, and aspect ratio. Regression analysis of data from this work and previous publications yielded an equation for predicting the ratio of the modulus of rupture (MOR) to the initial fracture strength. After cracking, carbon-fiber-reinforced cementitious composites (CFRCCs) were fragile, but their flexural strength was two to three times higher than that of control specimens. This was because the increased fiber volume and aspect ratio made the materials stronger and better at handling load and deflection.
This research investigates fiber-reinforced cementitious composites, with a particular emphasis on the geometric properties of soft micro and macro fibers. These fibers are characterized by a lower elastic modulus and larger aspect ratios than steel fibers. The composites were manufactured using a cement-to-sand ratio of 1:2.5, with 20% fly ash serving as a partial substitute. In order to attain varying strengths, two water-to-binder ratios (0.55 and 0.60) were implemented. Synthetic fibers, such as carbon and polypropylene, and natural sisal fibers, were introduced in volumes varying from 0.4% to 2.27%, with aspect ratios ranging from 71 to 3750. The flexural strength and behavior were evaluated using 75x75x380 mm prisms, while the compressive strength was measured using 50 mm cubes. Load-deflection curves were developed to investigate fracture behavior. The behavior of specimens reinforced with fibers post-cracking is dependent upon the matrix compressive strength, fiber type, quantity, and aspect ratio. A regression analysis was conducted on data from this study and previous publications to develop an equation that predicts the ratio of modulus of rupture (MOR) to initial fracture strength. The variables are matrix strength and fiber characteristics. The results reveal that carbon fiber-reinforced composites (CFRCCs) exhibit considerable brittleness post-cracking, despite exhibiting a flexural strength that is two to three times greater than that of control specimens. When workability is not compromised, the maximal load capacity and deflection are improved by increasing the fiber volume and aspect ratio. The maximal load stress is more significantly influenced by volumes of fibers than by aspect ratio.
The aim of this work is to investigate the effect of curing temperature and time on the development of compressive strength in geopolymer mortars produced using ground granulated blast-furnace slag (GGBFS) and fly ash (FA). Considering curing circumstances, both the activation energy and the reference temperature could be used properly to build a reliable anticipated model for predicting the compressive strength of geopolymer-based products (mortar and concrete) using maturity-based techniques. In this study, the compressive strength development of geopolymer mortar made from (FA) and (GGBFS) under varying curing conditions. The mortar was prepared using an alkali solution of sodium hydroxide (NaOH) and sodium silicate (Na2SiO3) in a 1:1 ratio, with NaOH molarity of 12. Specimens were cast following ASTM C109 standards, with a binder/sand ratio of 1:2.75, and compacted for full densification. FA-based mortar was cured at 40 °C, 80 °C, and 120 °C, while GGBFS-based mortar was cured at 5 °C, 15 °C, and 40 °C for durations of 0.5 to 32 days. Compressive strength was evaluated at each curing period, and data were analyzed using ASTM C1074 procedures alongside a computational model to determine the best-fit datum temperature and activation energy. The Nurse-Saul maturity method and Arrhenius equation were applied to estimate the equivalent age and maturity index of each mix. A predictive model was developed for geopolymer concrete prepared at an alkali-to-binder ratio of 0.45 and NaOH molarity of 12. The final equation demonstrated high accuracy, offering a reliable tool for predicting geopolymer strength under diverse curing conditions and providing valuable insights for optimizing geopolymer concrete formulations.
Strain-hardening geopolymer composites (SHGCs) have been introduced to address performance challenges in concrete construction. SHGCs are unique materials that exhibit strain-hardening behavior with multiple microcracks. There is a lack of studies on the inclusion of local sustainable materials and different aspect ratios of steel fiber hybridized with polyvinyl alcohol (PVA) fibers in this context. This study aims to address this gap by evaluating the potential of employing local metakaolin, steel slag, and high-silica sand as matrices in SHGCs. Additionally, investigate the effect of mono- and hybrid PVA/steel fibers (low and high aspect ratios) on the development of strain-hardening in SHGCs with enhanced mechanical strengths. A series of experiments was conducted, including compression, uniaxial tension, single-crack tension, and fracture toughness tests. The results demonstrated that the mono-PVA and hybrid-PVA/steel (13 mm) fiber-reinforced composite exhibited the highest strain capacities of 3.75% and 3.71%, respectively. The higher aspect ratio steel fiber exhibited 0.55% higher strain capacity than the mono-13 mm steel fibers. These composites demonstrated adequate micromechanical properties, enabling effective fiber bridging and energy dissipation. Moreover, higher aspect-ratio fibers significantly enhanced the mechanical properties of the mono-PVA-reinforced SHGC, particularly tensile and compressive strength by up to 265% and 79%, respectively. The potential of fiber-reinforced geopolymer mortars is demonstrated in these study findings as reliable strain-hardening composites for sustainable civil engineering applications.