We report the exploration of all-inorganic perovskite photodetectors based on stabilized CsPb0.922Sn0.078I3 nanobelts, which exhibit overall excellent performance with an ultrahigh detectivity up to 6.43 × 1013 Jones.
We report a facile BiBr 3 (DMSO) 2 adduct process to produce high-quality Cs 2 AgBiBr 6 films with large grains for the first time, which leads to an enhancement of over 40% on the PCE of Cs 2 AgBiBr 6 -based solar cells compared to that of the control sample.
Magnesium-rare earth (Mg-Re) alloys are very promising structural materials in lightweight industries, while the poor corrosion resistance limits their widespread application. In this work, to provide insights into the functions of precipitate characteristics on the corrosion behaviors of Mg-Re alloys, the influence of heat treatments on the corrosion behavior of Mg-11.46Gd-4.08Y-2.09Zn-0.56Zr alloy was investigated via an immersion test, electrochemical experiment and scanning electron microscope (SEM). The results showed that the corrosion rate of Mg-11.46Gd-4.08Y-2.09Zn-0.56Zr alloy specimens decreased by 17.58% and 20.44% after T5 and T6 heat treatment, respectively. In the heat-treated specimens, the corrosion did not extend further into the matrix but formed fine corrosion grooves along the extrusion direction. The improved homogeneity reduced the residual stress and the β’ precipitate introduced as a corrosion barrier after T5 and T6 heat treatment reduced the corrosion rate of the studied Mg alloy. In addition, the volume fraction of the long-period stacking-ordered (LPSO) phase decreased after heat treatment, which effectively reduced galvanic corrosion and enhanced the protective effect on the Mg matrix.
SiC particle (SiCp) size has been found to significantly influence the hot workability of particle-reinforced aluminum matrix composites (AMC). In this work, therefore, three types of SiCp/6013 composites with different SiCp sizes (0.7, 5 and 15 μm) were prepared and then subjected to isothermal hot compression tests. In addition, constitutive analysis, processing maps and microstructural characterizations were used to reveal the influence of SiCp size on the hot workability of SiCp/6013 composite. The results showed that the values of hot deformation activation energy Q increased with decreasing SiCp size. Specifically, at lower temperatures (e.g., 350 and 400 °C), the highest peak stress was shown in the AMC with SiCp size of 0.7 μm (AMC-0.7), while in the AMC with SiCp size of 5 μm (AMC-5) at higher temperatures (e.g., 450 and 500 °C). This is because a finer SiCp size would lead to stronger dislocation pinning and grain refinement strengthening effects, and such effects would be weakened at higher temperatures. Further, dynamic softening mechanisms were found to transform from dynamic recovery to dynamic recrystallization with increasing SiCp size, and the dynamic recrystallization occurred more easily at higher temperatures and lower strain rates. Consequently, the instability zones of the composites are all mainly located in the deformation region with lower temperature and higher strain rate, and smaller SiCp results in larger instability zones.