The relationship between the molecular structure characteristics of pectin and the sorption equilibrium with a copper solution was evaluated. The chemisorption processes were described using...
3 May 2023 in International Journal of Biological Macromolecules
The elaborated principles of nanoengineering of linen textile materials implement the techniques of spatially localized effects of protein catalysts on polymeric cellulose companions with selective splitting of impurity compounds without damaging technologically necessary nano-sized formations of binders in the fiber structure. The ranges of optimal values of the residual content in flax fiber prepared for spinning are identified on the basis of the analysis of the successive stages of enzymatic and peroxide treatments contribution to the breakdown of polymers and the differentiation of the influence of impurities on the yarn technological properties. The recommended level of residual pectin, lignin and hemicellulose (wt. %) is: after enzymatic treatment P1 = 1,0±0,1; L1 = 3,9±0,3; Hc1 = 11,0±1,0; after peroxide bleaching P2 = 0,4±0,05; L2 = 2,3±0,3; Hc2 = 7,5±0,5. The required level of fiber structural modification at the stage of preparing roving for spinning can be achieved through use of protein catalysts whose globule size is 50...100 nm. The use of enzymes with these dimensional characteristics helps to ensure breaking of polymer adhesives on the surface of incrusts and in the areas of intercellular formations, which hinder fiber crushing, without damaging nano-sized binding fractions. The implementation of this method contributes to a significant improvement in the uniformity of structural and physical and mechanical properties of flax yarn. Increase in yarn fineness and strength properties of semi-finished products, as well as improvement of deformation properties and reduction of yarn breakages during the spinning processes are achieved.
1 January 2012 in Russian Journal of Organic Chemistry
Concentration and temperature dependences of the redox potentials of neutral and alkaline solutions of glucose, mannose, galactose, galacturonic acid, and xylose were measured. Axial orientation of the secondary hydroxy groups in epimeric hexopyranoses, oxidation of C6 to carboxy group, and the lack of primary hydroxy group in going to aldopentopyranose favor increasing (in the order of listing) destabilization of their cyclic structure, formation of the oxo form, and thermally activated retro-aldol reaction of the latter in alkaline medium. This leads to enhancement of their reducing power and chemical reactivity toward 5,5′,7,7′-tetrabromoindigo.
1 January 2018 in Russian Journal of Applied Chemistry
The degree of immobilization of montmorillonite on flax fiber was determined experimentally, and the effect of the nonadditive increase in the sorption capacity of the biocomponent material was...
20 February 2019 in International Journal of Chemical Engineering
This paper was focused on the method to increase of the sorption properties in the flax fibrous material. This method was based on the original approach which includes the application of enzymatic catalysis as a destruction regulator of the polycarbohydrate components in the bast. The formed reaction products were used as reagents for reductive destruction of lignin. The changes in the fiber sorption capacity to the molecular markers were controlled after changing both the polymer composition of the fiber and the size of its pore. It was determined that the flax sorbents increase the adsorption of phenol vapors to 9–12 times and organic dyes from aqueous solutions to 4 times.