The phase transformations in an as-cast Fe-30Mn-8.8Al-0.3Si-0.15C steel were analyzed experimentally and numerically with a Calphad-based method during heat treatment. The nonequilibrium phases were determined using the Thermo-Calc Scheil module and the equilibrium phases with Themo-Calc based on the steel chemical composition. The precipitated phases were analyzed with TC-PRISMA using the chemical composition, nucleation site, and temperature among other factors. An ingot of this chemical composition was vacuum-melted using pure elements under an Ar gas atmosphere. As-cast steel specimens were annealed and solution-treated, quenched, and then aged at different temperatures. Heat-treated specimens were analyzed by different techniques. The results indicated that the microconstituents are the α and γ phases for the as-cast, homogenized, and quenched conditions. The main difference among these conditions is the distribution and size of the γ phase, which produced a change in hardness from 209 to 259 VHN. In contrast, the aging treatment at 750 °C caused a decrease in hardness from 492 to 306 VHN, which is attributable to the increase in volume fraction of the γ phase. On the other hand, the aging treatment at 550 °C promoted precipitation hardening from 259 to 649 VHN because of the κ precipitate formation. The calculated results for the different heat treatments with the Calphad-based method agreed well with the experimental ones. In addition, the intragranular precipitation of the κ phase could be simulated using the nucleation and growth and coarsening mechanisms based on a Calphad method.
The present work focused on analyzing the phase transformation in Fe-Ni-Al alloys employing a diffusion couple of Ni/Fe-Ni-Al/Fe, and Calphad-based diffusion and thermodynamic software. Diffusion couples were prepared by annealing at 1100 °C for 200 h and then air-cooled. These couples were also aged at 750 °C for 100 and 275 h. Both numerical and experimental results indicated that the diffusion path between Ni or Fe pure metal and the Fe-33at.%Ni-33at.%Al alloy is not linear. The phases formed during the diffusion anneal at 1100 °C correspond to those shown in the Calphad-calculated Fe-Ni-Al equilibrium diagram. The aging treatment at 750 °C promoted the inverse precipitation β′ → β′ + α, which caused the softening of the alloy. Moreover, the normal precipitation reactions, α→α + β′ and γ → γ + γ′, were also observed to occur during the aging of diffusion couple at 750 °C, originating precipitation hardening.