This numerical study investigates the impact of the reaction temperature, molar ratio of CH4:CO2, and catalyst porosity (εp) on the H2 yield and H2 selectivity during biogas dry reforming over a Ni/Cr catalyst. Using COMSOL Multiphysics, we conducted detailed simulations to elucidate the underlying reaction characteristics. Our findings reveal that increasing εp from 0.1 to 0.95 significantly provides a 5 times increase in H2 production and a 2.3% increase in H2 selectivity while simultaneously reducing CO selectivity by 2.3%. This effect is attributed to the improved mass transfer within the catalyst bed, leading to more efficient reactant conversion and product formation. Additionally, we observed a strong correlation between higher reaction temperatures and increased H2 yield and H2 selectivity. By optimizing these operational parameters, our results suggest that Ni/Cr catalysts can be effectively employed for the sustainable production of H2 from biogas.
The present study pays attention to biogas dry reforming for the purpose of producing H2. It is known that biogas contains approximately 40 vol% CO2, causing a decrease in the efficiency of power generation due to its lower heating value compared to natural gas, i.e., CH4. We suggest a hybrid system composed of a biogas dry reforming membrane reactor and a high-temperature fuel cell, i.e., a solid oxide fuel cell (SOFC). Since biogas dry reforming is an endothermic reaction, we adopt a membrane reactor, controlled by providing a non-equilibrium state via H2 separation from the reaction site. The purpose of the present study is to understand the effect of the thickness of the Pd/Cu membrane on the performance of the biogas dry reforming membrane reactor with a Pd/Cu membrane as well as a Ni/Cr catalyst. The impact of the reaction temperature, the molar ratio of CH4:CO2 and the differential pressure between the reaction chamber and the sweep chamber on the performance of the biogas dry reforming membrane reactor with the Pd/Cu membrane as well as the Ni/Cr catalyst was investigated by changing the thickness of the Pd/Cu membrane. It was revealed that we can obtain the highest concentration of H2, of 122,711 ppmV, for CH4:CO2 = 1:1 at a reaction temperature of 600 °C and a differential pressure of 0 MPa and using a Pd/Cu membrane with a thickness of 40 μm. Under these conditions, it can be concluded that the differential pressure of 0 MPa provides benefits for practical applications, especially since no power for H2 separation is necessary. Therefore, the thermal efficiency is improved, and additional equipment, e.g., a pump, is not necessary for practical applications.
This study proposes a combination system consisting of a biogas dry reforming reactor and a solid oxide fuel cell (SOFC). Since biogas dry reforming is an endothermic reaction, this study adopted a membrane reactor operated due to the non-equilibrium state with H2 separation from the reaction space. This study aimed to clarify the performance of the Ni/Cr/Ru catalyst using a biogas dry reforming membrane reactor. Additionally, this study also undertook a comparison of the performance of the Ni/Cr/Ru catalyst with that of the Ni/Cr catalyst. The impact of operation temperature, the molar ratio of CH4:CO2, the differential pressure between the reaction chamber and the sweep chamber, and the introduction of a sweep gas on the performance of the biogas dry reforming membrane reactor using a Pd/Cu membrane and a Ni/Cr/Ru catalyst was examined. The concentration of H2 using the Ni/Cr/Ru catalyst was greater than that using the Ni/Cr catalyst by 2871 ppmV for the molar ratio of CH4:CO2 = 1.5:1 at the reaction temperature of 600 °C and the differential pressure of 0 MPa without a sweep gas in particular. Under this condition, CH4 conversion, H2 yield, and thermal efficiency were 67.4%, 1.77 × 10−2%, and 0.241%, respectively.
This numerical study investigates the impact of reaction temperature, molar ratio of CH4:CO2, and catalyst porosity (p) on H2 yield and H2 selectivity during biogas dry reforming over a Ni/Cr catalyst. Using COMSOL Multiphysics, we conducted detailed simulations to elucidate the underlying reaction characteristics. Our findings reveal that increasing p significantly enhances H2 production and H2 selectivity, while simultaneously reducing CO selectivity. This effect is attributed to the improved mass transfer within the catalyst bed, leading to more efficient reactant conversion and product formation. Additionally, we observed a strong correlation between higher reaction temperatures and increased H2 yield and H2 selectivity, confirming the endothermic nature of the reforming process. By optimizing these operational parameters, our results suggest that Ni/Cr catalysts can be effectively employed for the sustainable production of H2 from biogas.
The aim of the present study was to clarify the influence of the thickness of the Pd/Cu membrane on the characteristics of biogas dry reforming (BDR) with aNi/Cr/Ru catalyst. We also clarified the impact of the reaction temperature, the molar ratio of CH4:CO2, the differential pressure between the reaction and sweep chambers, and the introduction of a sweep gas on the characteristics of a BDR reactor with a Pd/Cu membrane and a Ni/Cr/Ru catalyst. Through this study’s results, we clarify that the concentration of H2 in the reaction chamber and the sweep chamber increases with the increase in the reaction temperature. In addition, this study clarifies that the highest concentration of H2 in the reaction chamber and the sweep chamber can be obtained with a molar ratio of CH4:CO2 = 1.5:1. This study also clarifies that the highest concentration of H2 can be obtained with a thickness of 40 μm, a molar ratio of CH4:CO2 = 1.5:1, and a differential pressure between the reaction chamber and the sweep chamber of 0 MPa without a sweep gas, which was 4890 ppmV in the reaction chamber and 38 ppmV in the sweep chamber. Under these conditions, CH4 conversion, H2 yield, and thermal efficiency were 75.0%, 0.214%, and 2.92%, respectively.
This study proposed the combination system consisting of biogas dry reforming reactor and solid oxide fuel cell (SOFC). Since a biogas dry reforming is an endothermic reaction, this study adopted a membrane reactor operated due to the non-equilibrium state with H2 separation from the reaction space. This study aimed to clarify the characteristics of Ni/Cr/Ru catalyst using for a biogas dry reforming membrane reactor. Additionally, this study also investigated the comparison of the characteristics of Ni/Cr/Ru catalyst with that of Ni/Cr catalyst. The impact of operation temperature, the molar ratio of CH4 : CO2, the differential pressure between the reaction chamber and the sweep chamber and the introduction of sweep gas on the characteristics of the biogas dry reforming membrane reactor using Pd/Cu membrane and Ni/Cr/Ru catalyst was examined. The concentration of H2 using Ni/Cr/Ru catalyst was larger than that using Ni/Cr catalyst by 2871 ppmV for the molar ratio of CH4 : CO2 = 1.5 : 1 at the reaction temperature of 600 ℃ and the differential pressure of 0 MPa without a sweep gas, especially. Under this condition, CH4 conversion, H2 yield and thermal efficiency were 67.4 %, 1.77×10-2 % and 0.241 %, respectively.