Graphene oxide (GO) has attracted significant attention as a nano-reinforcement for cement-based materials, owing to its exceptional mechanical properties and abundant surface functional groups. However, the precise mechanisms governing its effects in cement composites remain inadequately understood due to inconsistencies and gaps in the existing literature. This review conducts a comprehensive analysis of the dispersion and reinforcement effects of GO in cement materials, focusing on three key areas: (1) challenges associated with achieving uniform dispersion of GO in the high-pH environment of cement slurries and potential strategies to address them; (2) the influence of GO on the macroscopic properties of cementitious composites, including workability, load-bearing capacity, flexural strength, fracture resistance, and durability; and (3) the reinforcement mechanisms of GO, encompassing its role in hydration kinetics, alterations to the calcium-silicate-hydrate (C-S-H) structure, and bonding interactions at the cement matrix interface. Furthermore, recent advancements in optimizing the dispersion and reinforcement effects of GO, such as surface modification techniques, are explored, emphasizing its potential for multifunctional and intelligent applications. This review aims to provide engineering professionals with the latest insights into the application of graphene oxide as a nano-reinforcement in cement-based composites, while offering valuable guidance and direction for future research in this field.
Foam concrete is highly valued as a sustainable cement-based material, but the development of 3D-printed foam concrete (3DPFC) has remained constrained. This study investigated the influence of printing interval on the microstructure and imbibition behavior of 3DPFC. The results revealed that horizontal interlayers are broader compared to vertical interlayers, leading to more significant imbibition. For X-oriented 3DPFC, the vertical interlayer was rapidly occupied by water after imbibition, forming an elliptical moisture profile. For Y-oriented 3DPFC, the moisture profile appeared more convoluted, mainly surrounding the horizontal interlayers but shifting at intersections with the vertical interlayers. In Z-oriented 3DPFC, where only tight horizontal interlayers were present, interlayer imbibition was almost negligible. Additionally, when the printing interval was less than 15 min, imbibition was primarily restricted to the top filament since the bottom filament was compacted by the filament above. Conversely, with a printing interval longer than 15 min, the bottom filament hardened before the setting of the top filament. This allowed the surface of the bottom filament to be compacted by the top filament, resulting in a dense interlayer that offers better resistance against imbibition compared to the matrix of 3DPFC. This work contributes to the advancement of green building technologies by providing insights into optimizing the 3D printing process for foam concrete, thereby enhancing its structural performance without compromising the designated air content and consistency of the foam concrete, facilitating a more efficient utilization of materials and a reduction in overall material consumption.
Wood is a renewable and sustainable environmentally friendly building material. With proper design, it can help buildings achieve lower carbon emissions. However, since wood is a flammable material, its combustion performance in fires has attracted attention. In modern timber structures, glulam is a widely used engineered wood product. Thus, in this paper, glulam specimens made of four kinds of commonly used soft-wood species were used to compare their combustion performance, and the cone calorimeter method was employed. The indicators including time to ignition, heat release rate per unit area, total heat release per unit area, specific extinction area per unit mass, mass of residue, yield of CO and yield of CO2 were evaluated and compared. The results showed that all the glulam specimens would experience cracking wood and adhesive layer. The time to ignition and peak mass loss rate of the four softwood species in the study was positively correlated with their density. Among these species, Spruce exhibited the highest peak heat release rate and the highest peak CO2 yield but lowest smoke production, while Douglas fir had a relatively late CO production time and the lowest mass loss percentage, Larch had the lowest heat release rate and total heat release. This study provides fundamental data for the selection of wood structural materials and for future research on wood flame-retardant treatments.