Engineering Research Centre for Waster Oil Recovery Technology and Equipment of Ministry of Education, Chongqing Technology and Business University, Chongqing 400067, China
Dr. Weiyan Jiang
Engineering Research Centre for Waster Oil Recovery Technology and Equipment of Ministry of Education, Chongqing Technology and Business University, Chongqing 400067, China
A gradient Mg-8 wt % Si alloy, which was composed of the agglomerated Mg2Si crystals coating (GMS8-1) and the eutectic Mg–Si alloy matrix (GMS8-2), was designed for biodegradable orthopedic implant materials. The bio-corrosion behavior was evaluated by the electrochemical measurements and the immersion tests. The results show that a significant improvement of bio-corrosion resistance was achieved by using the gradient Mg–Si alloy, as compared with the traditional Mg-8 wt % Si alloy (MS8), which should be attributed to the compact and insoluble Mg2Si phase distributed on the surface of the material. Especially, GMS8-1 exhibits the highest polarization resistance of 1610 Ω, the lowest corrosion current density of 1.7 × 10−6 A·cm−2, and the slowest corrosion rate of 0.10 mm/year. In addition, GMS8-1 and GMS8-2 show better osteogenic activity than MS8, with no cytotoxicity to MC3T3-E1 cells. This work provides a new way to design a gradient biodegradable Mg alloys with some certain biological functions.
The morphology evolution of long-period stacking ordered (LPSO) phases on corrosion behavior of Mg95.33Zn2Y2.67 alloy is investigated systematically during as-cast, pre-extrusion heat-treated, as-extruded and post-extrusion heat-treated conditions. The second phases in the as-cast alloy are only LPSO phases with a few Y particles. The pre-extrusion heat treatment changed LPSO phases from blocks into a rudimentary rod shape with lamellar structure, subsequently into fine fragments by extrusion, and then into a regular rod shape with lamellar structure followed by post-extrusion heat treatment. Immersion tests and electrochemical measurements in 3.5 wt % NaCl solution reveal that the post-extrusion heat-treated alloy has the best corrosion resistance with the lowest corrosion rate. This is attributed to the rod-shaped LPSO phases, which could hinder corrosion proceeding, and result in corrosion orientated along the direction of rods and forming relatively dense long-strip corrosion products. Our findings demonstrate that the improved corrosion resistance of magnesium alloys with LPSO phases can be tailored effectively by the proceeding technology and post-heat treatment.