Qiangqiang Liao

Qiangqiang Liao


Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
12 December 2019 in International Journal of Energy Research
Verified
Journal Article
Closed access
PDF file
XLXinzhou Li
Xinzhou Li
LZLizhong Zhang
Lizhong Zhang
YLYi Liu
Yi Liu
APAiqiang Pan
Aiqiang Pan
QLQiangqiang Liao
Qiangqiang Liao
XYXiu Yang
Xiu Yang

27 December 2018 in International Journal of Energy Research
Verified
Journal Article
Closed access
PDF file
QLQiangqiang Liao
Qiangqiang Liao
YZYoulang Zhang
Youlang Zhang
YTYibin Tao
Yibin Tao
JYJilei Ye
Jilei Ye
CLCheng Li
Cheng Li

1 September 2021 in Sustainable Chemistry and Pharmacy
Verified
Journal Article
Closed access
LMLinrui Ma
Linrui Ma
WLWenqing Lu
Wenqing Lu
DYDong Yang
Dong Yang
JSJianjia Shen
Jianjia Shen
ZGZesong Gao
Zesong Gao
QLQiangqiang Liao
Qiangqiang Liao

2 September 2016 in Corrosion Reviews
Verified
Journal Article
Closed access
PDF file
DYDong Yang
Dong Yang
SLSong Hui Liu
Song Hui Liu
YSYu Pei Shao
Yu Pei Shao
SXShao Di Xu
Shao Di Xu
LZLu Lu Zhao
Lu Lu Zhao
HGHong Hua Ge
Hong Hua Ge
The corrosion inhibition behavior of an imidazoline derivative, namely, 2-undecyl- N -carboxymethyl- N -hydroxyethyl imidazoline (UHCI) for carbon steel in 4 wt.% citric acid solutions was characterized by weight loss method and electrochemical techniques in conjunction with X-ray photoelectron spectrometer (XPS) technique. The inhibitor has a good anti-corrosion effect on the carbon steel in 4 wt.% citric acid solutions. The inhibition efficiency increases with UHCI concentrations from 0 up to 0.4 wt.%, yet declines a bit at 0.6 wt.% per contra with further augmentation of concentration. The inhibition efficiency declines with the rise of temperature from 20°C to 95°C, while it rises with the extension of soaking time from 2 h to 24 h. Two N 1s peaks that appeared in XPS spectra give proof of UHCI inhibitor adsorbed on the carbon steel surface.

28 February 2017 in Journal of Materials Engineering and Performance
Verified
Journal Article
Closed access
PDF file
YSYupei Shao
Yupei Shao
MMMiaomiao Mu
Miaomiao Mu
BZBing Zhang
Bing Zhang
KNKaibin Nie
Kaibin Nie
QLQiangqiang Liao
Qiangqiang Liao

21 August 2017 in Corrosion Reviews
Verified
Journal Article
Closed access
PDF file
MMMiaomiao Mu
Miaomiao Mu
YCYaqiong Chen
Yaqiong Chen
DYDong Yang
Dong Yang
AYAijun Yan
Aijun Yan
QLQiangqiang Liao
Qiangqiang Liao
The mixture of 2-undecyl- N -carboxymethyl- N -hydroxyethly imidazoline (UHCI) with potassium iodide (KI) as a corrosion inhibitor for carbon steel in 8% amidosulfuric acid solution was investigated by weight loss test and electrochemical methods. Results show that the combined inhibitor strongly inhibits the corrosion of 20# carbon steel in amidosulfuric acid solution, and the mixture with the mass ratio (UHCI:KI) of 9:1 has the best corrosion inhibition at a total concentration of 0.4%. The impedance spectra of carbon steel electrodes change from one time constant into two time constants when the mixture inhibitor adds into the blank solution, while the polarization curves indicate that the mixture behaves as a mixed type inhibitor. The mixture is found to follow the Langmuir adsorption isotherm, and the mechanism is chemisorption.