Norway spruce (Picea abies (L.) H.Karst) trees planted with high stem densities produce finely branched, solid logs but are vulnerable to extreme weather events, e.g., storms. Over the last decades spruce stands have been planted at lower stand densities, resulting in wider crowns, lower crown bases, and higher stand stability, but this might decrease the quality of coniferous timber due to an increased growing rate and wider annual rings. Therefore, in this case study we investigated the influence of different silvicultural treatments and stand densities on tree morphology and wood properties of 100 spruce trees up to sawn timber as the final product. Tree morphology was assessed using mobile laser scanning. Ring width analysis, wood density measurements, and the four-point bending strength test on visually graded boards were conducted to gain information on wood properties and product quality. In stands thinned from below, higher wood densities were observed due to smaller annual rings compared to stands that were thinned from above at equal annual ring widths. In addition, crown asymmetry and the height-to-diameter ratio were identified as proxies for wood density. Lastly, visually assessed quality differences between the forest stands were discerned on the examined boards.
A study was conducted to improve the effectiveness of silvicultural production of structural sawn timber from softwoods. It intends to explore prediction methods for mechanical timber quality. The study material was obtained from six stands divided into age groups of approximately 40- and 80-year-old trees (examining the influence of age). The stands were differentiated by their applied thinning system of thinning from below or above (examining the influence of the thinning system). Resulting from these different levels of data, i.e., stand parameters, tree anatomy, and visual board properties are examined and analyzed in ordinal logistic models and linear mixed models. Visual board properties were discerned by means of the German standard for visual grading of sawn timber. The mechanical board properties were measured in on-edge bending strength tests and allocated into strength classes, which were modeled in dependence of visual characteristics and forestry conditions. The evaluation of mechanical properties attributed a significant loss of timber quality to short rotation periods, non-ideal water supply, and a single-tree management system. The prediction capabilities of models based on site and tree characteristics were on par with the accuracy of visual grading. Management adaptations by intense thinning from above can lead to a significant decline in Norway spruce (Picea abies L.) timber quality when site factors coincide. Particular care should be taken in the management of locations with high yield potential. Non-destructive evaluation based on site characteristics combined with terrestrial laser scan data of tree characteristics has potential as a pregrading method.
This study evaluates the potential of various hardwood combinations in plywood production in response to increasing wood demand and a changing roundwood supply in Central Europe. Six different combinations of nine-layer plywood were produced using 2 mm rotary-cut veneers from lime (Tilia spp.), Norway maple (Acer platanoides), European hornbeam (Carpinus betulus), Sycamore maple (Acer pseudoplatanus), mountain ash (Sorbus aucuparia), and European beech (Fagus sylvatica) with phenol–formaldehyde adhesive, and they were compared to silver birch (Betula pendula) plywood as a reference. The raw densities of the test panels varied between 0.85 and 1.04 times the reference density (795 kg m−3). Flexural strengths (the modulus of rupture, MOR) ranged from 68 N mm−2 to 104 N mm−2 for a parallel fibre orientation and 44 N mm−2 to 61 N mm−2 for a perpendicular fibre orientation of the top layers. The modulus of elasticity (MOE) ranged from 7160 N mm−2 to 11,737 N mm−2 for the parallel fibre orientation and from 4366 N mm−2 to 5575 N mm−2 for the perpendicular orientation. The tensile shear strength varied between 0.91 and 1.69 times the reference (1.49 N mm−2). The thickness swelling after 24 h was higher in all variants than the reference (6.4%), with factors between 1.39 and 1.64. A significant effect was observed when layers with a lower density were arranged on the outside and those with a higher density in the core, resulting in a more uniform density distribution across the cross-section after hot pressing. This created a levelling effect on mechanical and physical properties, especially the modulus of rupture (MOR) and the modulus of elasticity (MOE). Overall, the evaluated hardwood combinations demonstrated comparable properties to the birch reference and industrially produced birch plywood.
The relationship between silvicultural strategies, manifested in the thinning method and rotation age on sites with different water supply, and the mechanical properties of engineered wood products plywood and laminated veneer lumber has been analyzed. Sample logs from five German sites of Norway spruce (Picea abies (L.) Karst.) and Douglas fir (Pseudotsuga menziesii (M.) Franco) have been rotary-peeled and processed into boards with a phenol–resorcinol–formaldehyde adhesive to evaluate their performance under flexural, tensile, and compressive loads. Satisfactory coefficients of determination were reached for Norway spruce in regard to the silvicultural framework and the tree characteristics of slenderness and crown base height. Douglas fir products did not achieve comparable determination due to high variance within boards and stands but did achieve significantly better mechanical properties. Norway spruce was observed to be more responsive to thinning measures, while the effect of different thinning regimes was not evident for Douglas fir. The on-site evaluation of Douglas fir stands for veneer product quality based on silvicultural parameters and tree characteristics was shown to be inconclusive, with its naturally higher wood density being the decisive constant.