Active brazing of zirconia with metallic alloys is a promising method for enhancing the mechanical property of zirconia. However, the brazing process of zirconia and metallic alloys has not been studied in detail because of a limitation in selection of materials and processing conditions. Here, we successfully brazed zirconia with Ti-3Al-2.5V alloy using amorphous Zr54Ti22Ni16Cu8 active filler alloy. By manipulating the brazing temperature from 800 °C to 860 °C, a highest strength of ~186 MPa was achieved at 860 °C. Reduced brittle (Zr,Ti)2(Ni,Cu) intermetallic phases from formation of island-type (Zr,Ti) matrix, ZrO2-X, TiO, and TiO2 interlayer play a key role in increasing the joint strength. Our findings will be helpful in developing brazing processes for zirconia and metallic alloys.
Binder-jetted metallic components retain residual porosity after sintering, which can substantially affect their mechanical and tribological performance. This study clarifies how sintering-induced pore evolution and Cu infiltration influence the wear mechanisms of binder-jetted STS316L. STS316L specimens were sintered at 1100, 1200, and 1300 °C, and corresponding Cu/STS316L composites were fabricated by molten Cu infiltration. Their microstructures and wear behavior were analyzed using Filed-emission scanning electron microscopy (FE-SEM), Energy-dispersive X-ray spectroscopy (EDS), Confocal laser scanning microscopy (CLSM), X-ray diffraction (XRD), and cross-sectional Transmission electron microscopy (TEM). As the sintering temperature increased, the relative density and hardness of the sintered specimens increased from 72.75% to 80.69% and from 194 to 243.8 HV, respectively. Nevertheless, their average coefficient of friction increased from approximately 0.25 to 0.71, while the wear width and maximum depth increased from 932.8 to 1492.0 μm and from 24.7 to 60.3 μm, respectively. Abrasive and adhesive wear predominated at 1100 and 1200 °C, whereas repeated formation, cracking, and delamination of an approximately 2.5 μm thick oxygen-rich tribolayer caused severe oxidative delamination at 1300 °C. Cu infiltration increased the relative density to 90.68–95.69%. The composites exhibited similar friction behavior, with an average coefficient of friction of approximately 0.6, and were governed primarily by adhesive wear associated with Cu transfer and plastic deformation. These results demonstrate that increased densification does not necessarily improve wear resistance and that pore structure and Cu transfer critically determine the dominant wear mechanisms.
In this study, the applicability of an Al-Si alloy with 30 wt% added scrap for automobile pistons was evaluated by investigating the melt quality, microstructural characteristics, and tensile properties under modified GBF (gas bubbling filtration) process conditions, including increasing rotor rotation speed and adjusting the air-line supply and the inclination angle of the impeller blade. The melt quality was dramatically improved under modified GBF process conditions, resulting in a very clean melt, with the D.I. value decreasing by 28%, the length of the oxide layer per kilogram decreasing by 65%, and inclusion content decreasing by 97% compared to that of the conventional GBF process conditions. Additionally, the size of primary Si decreased from 40 µm to 27 µm, and the eutectic Si and intermetallic compounds were refined, showing a very fine microstructure. The identified phases included Al4Cu2Mg8Si7, AlxCuyNiz, and MgO. The ultimate tensile strength was 275 MPa, and the elongation was 6.0%, indicating improved tensile properties compared to those of the conventional GBF process conditions. The fracture behavior changed from a brittle microcleavage fracture mode to a ductile dimple fracture mode as the primary Si, eutectic Si particles, and intermetallic compounds were refined under modified GBF process conditions. These results confirmed that Al-Si alloy with added scrap can be used as a material for automobile pistons.