Cold-formed steel (CFS) sections have become popular in construction due to several advantages over structural steel. However, research on the performance of galvanized iron (GI)-based CFS under high temperatures, especially regarding its flexural behavior, has been limited. This study extensively investigates how GI-based CFS beams with varying spans behave under elevated temperatures and subsequent cooling using air and water. This study examines the impact of temperature loading and compares the effectiveness of air- and water-cooling methods. Experimental results are validated and analyzed alongside findings from finite element modeling (FEM) using ABAQUS (2019_09_13-23.19.31) and the Direct Strength Method (DSM). Additionally, this study conducts a parametric investigation to assess how beam span influences flexural capacity. Among beams heated to the same temperature, those cooled with water show slightly lower load capacities compared to those cooled with air. The highest load capacity observed is 64.3 kN for the reference specimen, while the lowest is 26.2 kN for the specimen heated for 90 min and cooled with water, a 59.27% difference between them. Stiffness decreases as heating duration increases, with the reference section exhibiting significantly higher stiffness compared to the section heated for 90 min and cooled with water, with a 92.76% difference in stiffness. As heating duration increases, ductility also increases. Various failure modes are observed based on different heating and cooling conditions across different beam spans. This study provides insights into how GI-based CFS beams perform under temperature stress and different cooling scenarios, contributing valuable data for structural design and safety considerations in construction.
Cold-formed steel (CFS) sections, increasingly favored in the construction industry due to their numerous advantages over hot-rolled steel, have received limited attention in research concerning the flexural behavior of galvanized iron (GI)-based CFS at elevated temperatures. Understanding how these materials and structures behave under elevated temperatures is crucial for fire safety. The authors have performed experimental studies previously on GI-based CFS under elevated temperatures. In that study, CFS sections made of GI of grade E350 of 1.5 m long and 2 mm thickness were used. Built-up beam sections were tested under two-point loading after heating to 60 and 90 min durations and subsequently cooling them down using air and water. This study aims to uncover the influence of different stiffener configurations on the load carrying capacity of sections under elevated temperature parametrically. With the experimental study results from previous studies as a reference, authors used FEM analysis to comprehensively study the behavior of GI-based CFS sections under fire. Vertical, horizontal, and not providing a stiffener were the configurations selected to study the beams parametrically. Parametric analysis confirmed that different stiffener configurations did not alter the predominant failure mode, which remained distortional buckling across all specimens. Beams with vertical stiffeners demonstrated superior performance compared to those with horizontal stiffeners in parametric analysis. Lateral–torsional buckling was observed in the reference specimen, lacking stiffeners due to inadequate restraint at the supports.
31 March 2024 in Electronic Journal of Structural Engineering
Cold-formed steel (CFS) sections are used to construct medium and low-rise structures designed to carry small-scale loads. CFS sections are manufactured without the application of heat. Therefore, it is crucial to comprehend the properties of CFS sections which are exposed to fire or elevated temperatures. To simulate the real- time fire exposure, an ISO Standard fire curve was used to heat the CFS sections. The objective of the study is to assess the residual mechanical strength of exposed sections after the elevated temperature test. The study aims to compile data for forecasting the degeneration of elements and to ascertain whether the structural components can be reused or replaced. The CFS sections were subjected to different temperatures, and after heating, two cooling methods were used to bring down to room temperature. The characteristics of the retrieved specimens, taken from exposed CFS sections were assessed using a tensile coupon test. The residual properties such as ultimate strength, yield strength, and elastic modulus were examined and reported. The influence of heating and cooling is more pronounced from the test results. A reduction in the yield and ultimate strength was noticed, and it was found to decrease as the heating intensity increases for air and water cooling respectively. In the case of yield and ultimate strength, the strength reduction is critical beyond 60 minutes. The elastic modulus was also found to be reducing with a similar trend. Based on the test results, reduction factors are proposed for ultimate strength, yield strength and elastic modulus. Reduction factors obtained for yield strength under 60 minutes of heating for air and water cooling is 0.575 and 0.557 respectively. In 120 minutes, the values are 0.400 and 0.329. Reduction factors obtained for ultimate strength under 60 minutes of heating for air and water cooling is 0.586 and 0.566 respectively. For 120 minutes, the values are 0.331 and 0.313.
10 November 2023 in Journal of Structural Fire Engineering
Purpose: The capability of steel columns to support their design loads is highly affected by the time of exposure and temperature magnitude, which causes deterioration of mechanical properties of steel under fire conditions. It is known that structural steel loses strength and stiffness as temperature increases, particularly above 400 °C. The duration of time in which steel is exposed to high temperatures also has an impact on how much strength it loses. The time-dependent response of steel is critical when estimating load carrying capacity of steel columns exposed to fire. Thus, investigating the structural response of cold-formed steel (CFS) columns is gaining more interest due to the nature of such structural elements.Design/methodology/approach: In this study, experiments were conducted on two CFS configurations: back-to-back (B-B) channel and toe-to-toe (T-T) channel sections. All CFS column specimens were exposed to different temperatures following the standard fire curve and cooled by air or water. A total of 14 tests were conducted to evaluate the capacity of the CFS sections. The axial resistance and yield deformation were noted for both section types at elevated temperatures. The CFS column sections were modelled to simulate the section's behaviour under various temperature exposures using the general-purpose finite element (FE) program ABAQUS. The results from FE modelling agreed well with the experimental results. Ultimate load of experiment and finite element model (FEM) are compared with each other. The difference in percentage and ratio between both are presented.Findings: The results showed that B-B configuration showed better performance for all the investigated parameters than T-T sections. A noticeable loss in the ultimate strength of 34.5 and 65.6% was observed at 90 min (986℃) for B-B specimens cooled using air and water, respectively. However, the reduction was 29.9 and 46% in the T-T configuration, respectively.Originality/value: This research paper focusses on assessing the buckling strength of heated CFS sections to analyse the mode of failure of CFS sections with B-B and T-T design configurations under the effect of elevated temperature.
This study investigates the buckling performance of built-up cold-formed steel (CFS) columns, with a focus on how different thermal exposures and cooling strategies influence their susceptibility to various failure mechanisms. Addressing the gap in the literature on the fire behavior of mild steel (MS)-based CFS columns, the research aims to provide new insights. Compression tests were conducted on MS-based CFS column specimens after they were exposed to fire, to assess their post-fire buckling strength. The columns were subjected to controlled fire conditions following standardized protocols and then allowed to cool to room temperature. The study examined axial load-bearing capacity and deformation characteristics under elevated temperatures. To improve fire resistance, protective coatings—gypsum, perlite, and vermiculite—were applied to certain specimens before testing, and their performance was compared to that of uncoated specimens. A comprehensive finite element analysis (FEA) was also performed to model the structural response under different thermal and cooling scenarios, providing a detailed comparison of the coating effectiveness, which was validated against experimental results. The findings revealed significant variations in axial strength and failure mechanisms based on the type of fire-resistant coating used, as well as the heating and cooling durations. Among the coated specimens, those treated with perlite showed the best performance. For example, the air-cooled perlite-coated column (MBC2AC) retained a load capacity of 277.9 kN after 60 min of heating, a reduction of only 6.0% compared to the unheated reference section (MBREF). This performance was superior to that of the gypsum-coated (MBC1AC) and vermiculite-coated (MBC3AC) specimens, which showed reductions of 3.6% and 7.9% more, respectively. These results highlight the potential of perlite coatings to enhance the fire resistance of CFS columns, offering valuable insights for structural fire design.
8 July 2024 in Journal of Structural Fire Engineering
Purpose: Cold-formed steel (CFS) sections are a popular choice for constructing medium and low-rise structures that are engineered to support relatively light loads. An important characteristic of CFS sections is that they are produced without the use of heat during manufacturing. Consequently, it becomes essential to gain a comprehensive understanding in the behavior of CFS sections when exposed to fire or elevated temperatures.Design/methodology/approach: In this study, sections of 1.5 m length and 2 mm thickness were taken and analyzed to find its flexural behavior after heating them for 60 and 90 min. There were two modes of cooling phase which was considered to reach ambient temperature, i.e. air or water respectively. Performance of each sections (C, C with inclined flanges, sigma and Zed) were examined and evaluated at different conditions. Effects of different profiles and lips in the profiles on flexural behavior of CFS sections were investigated fully analytically.Findings: The variation in stiffness among the sections with different lipped profiles was noted between 20.36 and 33.26%, for 60 min water cooling case. For the sections with unlipped profiles, it was between 23.56 and 28.60%. Influence of lip and section profile on reduction in stiffness is marginal. The average reduction in load capacity of sections for 60 min specimens cooled by water was found to be 43.42%. An increase in deflection is observed for the sections in the range of 25–37.23% for 60 min case. This is the critical temperature responsible for reduction in yield strength of material as it substantially increases the material safety margin to be considered for the design. Sections with Zed profile have shown better performance among other types, in terms of its load carrying capacity.Originality/value: This paper deals with the flexural behavior of Galvanized (GI) based CFS unsymmetric sections at elevated temperature and cooled down to ambient temperature with air or water.