An InGaAs/GaAs quantum well (QW) structure was prepared by metal-organic chemical vapor deposition (MOCVD) via a new growth method, where the InGaAs well layer and the GaAs barrier layer were grown under a variable temperature. A GaAs protection layer was employed to avoid indium atom evaporation on the InGaAs surface during the temperature change. Room and low-temperature photoluminescence (RT/LT-PL), atomic force microscopy (AFM), and high-resolution X-ray diffraction (HRXRD) were carried out to investigate the effect of the variable temperature growth method. The theoretical and experimental results indicated that it could erase the 2D islands and rebuild the surface morphology to a step-flow mode surface. The quality of the InGaAs crystal layer was also improved because of the annealing-like treatment. In addition, the study found that when the thickness of the GaAs protection layer was 2 nm and the growth temperature of the InGaAs layer was 560°C, the maximal properties of the InGaAs/GaAs QW were achieved. Moreover, high-quality multiple QWs with five periods were grown with the tailored structure. The growth method will improve the properties of strained InGaAs/GaAs QW materials and provide technical support for a semiconductor laser's performance optimization.
InGaAs/InAlGaAs multiple quantum wells (MQWs) are widely adoped as the active region of near‑infrared semiconductor lasers due to their excellent optical performance and broad application prospects. In this work, we systematically investigate the effects of the thickness of a GaAs insertion layer (ISL) on the photoluminescence (PL) behavior and defect-associated carrier recombination dynamics of InGaAs/InAlGaAs MQWs. Through comprehensive structural characterization and temperature- and power-dependent PL spectroscopy, we demonstrate that a 2 nm-thick GaAs ISL provides optimal optical performance. All measured samples exhibit a distinctive S-shaped temperature evolution of the PL peak energy, a characteristic feature arising from carrier thermal redistribution among defect-induced localized states. Notably, the sample with a 2 nm GaAs ISL shows significantly suppressed localized states, accompanied by drastically improved radiative efficiency and overall crystal quality. These findings offer essential guidance for defect-aware structural design and performance optimization of InGaAs/InAlGaAs MQW heterostructures integrated with GaAs ISLs.