Graphene was grown on the C-face of nominally on-axis SiC substrates using high-temperature sublimation with Ar as the buffer inert gas. The results of studies of the morphology, thickness, and electronic structure of these samples using low-energy electron microscopy (LEEM), x-ray photoelectron emission microscopy, photoelectron spectroscopy, angle-resolved photoelectron spectroscopy (ARPES), and low-energy electron diffraction (LEED) are presented. The graphene thickness is determined to vary from 1 or 2 to 6 or 7 monolayers (MLs), depending on the specific growth conditions utilized. The formation of fairly large grains (i.e., crystallographic domains) of graphene exhibiting sharp 1\ifmmode\times\else\texttimes\fi{}1 spots in micro-LEED is revealed. Adjacent grains are found to show different azimuthal orientations. Macro-LEED patterns recorded mimic previously published, strongly modulated, diffraction ring LEED patterns, indicating contribution from several grains of different azimuthal orientations. We collected selected area constant initial energy photoelectron angular distribution patterns that show the same results. When utilizing a small aperture size, one Dirac cone centered on each of the six K-points in the Brillouin zone is clearly resolved. When using a larger aperture, several Dirac cones from differently oriented grains are detected. Our findings thus clearly show the existence of distinct graphene grains with different azimuthal orientations; they do not show adjacent graphene layers are rotationally disordered, as previously reported for C-face graphene. The graphene grain size is shown to be different on the different samples. In some cases, a probing area of 400 nm is needed to detect the grains. On one sample, a probing area of 5 $\mu${}m can be used to collect a 1\ifmmode\times\else\texttimes\fi{}1 LEED pattern from a multilayer graphene grain. ARPES is used to determine the position of the Dirac point relative to the Fermi level on two samples that LEEM shows have dominant coverage of 2 and 3 MLs of graphene, respectively. The Dirac point is found to be located within 75 meV of the Fermi level on both samples, which indicates that the electron carrier concentration induced in the second and third graphene layers on the C-face is less than $\sim${}4\ifmmode\times\else\texttimes\fi{}1011 cm$-${}2. Formation of patches of silicate is revealed on some samples, but the graphene formed on such nonhomogenous surfaces can contain fairly large ordered multilayer graphene grains.
Only a single linearly dispersing π-band cone, characteristic of monolayer graphene, has so far been observed in Angle Resolved Photoemission (ARPES) experiments on multilayer graphene grown on C-face SiC. A rotational disorder that effectively decouples adjacent layers has been suggested to explain this. However, the coexistence of μm-sized grains of single and multilayer graphene with different azimuthal orientations and no rotational disorder within the grains was recently revealed for C-face graphene, but conventional ARPES still resolved only a single π-band. Here we report detailed nano-ARPES band mappings of individual graphene grains that unambiguously show that multilayer C-face graphene exhibits multiple π-bands. The band dispersions obtained close to the moreover clearly indicate, when compared to theoretical band dispersion calculated in the framework of the density functional method, Bernal (AB) stacking within the grains. Thus, contrary to earlier claims, our findings imply a similar interaction between graphene layers on C-face and Si-face SiC.
Graphene grown on C-face SiC substrates using two procedures, high and low growth temperature and different ambients, was investigated using Low Energy Electron Microscopy (LEEM), X-ray Photo Electron Electron Microscopy (XPEEM), selected area Low Energy Electron Diffraction (μ-LEED) and selected area Photo Electron Spectroscopy (μ-PES). Both types of samples showed formation of μm-sized grains of graphene. The sharp (1 × 1) μ-LEED pattern and six Dirac cones observed in constant energy photoelectron angular distribution patterns from a grain showed that adjacent layers are not rotated relative to each other, but that adjacent grains in general have different azimuthal orientations. Diffraction spots from the SiC substrate appeared in μ-LEED patterns collected at higher energies, showing that the rotation angle between graphene and SiC varied. C 1s spectra collected did not show any hint of a carbon interface layer. A hydrogen treatment applied was found to have a detrimental effect on the graphene quality for both types of samples, since the graphene domain/grain size was drastically reduced. From hydrogen treated samples, μ-LEED showed at first a clear (1 × 1) pattern, but within minutes, a pattern containing strong superstructure spots, indicating the presence of twisted graphene layers. The LEED electron beam was found to induce local desorption of hydrogen. Heating a hydrogenated C-face graphene sample did not restore the quality of the original as-grown sample.
23 September 2013 in Journal of Materials Research