A β-solidifying Ti–43Al–2Cr–2Mn–0.2Y alloy was directionally solidified by the optical floating zone melting method. The microstructure is mainly characterized by γ/α2 lamellae with specific orientations, which exhibits straight boundaries. The β phase is randomly distributed in the lamellar microstructure, indicating that the β phase cannot be directionally solidified. The directional solidification of γ/α2 lamellae was not affected by the precipitation of the β phase. Hot compression tests show that the deformation behavior of the β-containing lamellar microstructure also exhibits the anisotropic characteristic. The deformation resistance of the lamellae is lowest when the loading axis is aligned 45° to the lamellar interface. Microstructural observation shows that the decomposition of the lamellar microstructure tends to begin around the β phase, which benefits from the promotion of a soft β phase in the deformation. Moreover, the deformation mechanism of the lamellar microstructure was also studied. The bulging of the γ phase boundaries, the decomposition of α2 lamellae and the disappearance of γ/γ interfaces were considered as the main coarsening mechanisms of the lamellar microstructure.
27 May 2016 in Journal of Mechanical Science and Technology
This study systematically investigated the influence of multi-directional forging (MDF) on the microstructural evolution, hot deformation behavior, and tensile properties of a β-solidifying TiAl alloy. The initial lamellar microstructure of an as-cast alloy was remarkably refined and homogenized by three-step MDF. High temperatures and multi-pass deformations were conducive to the decomposition of lamellae. A crack-free billet was obtained through three-step MDF, with a deformation temperature of 1250 °C and a forging speed of 0.1 mm/s, indicating that MDF can be applied to β-solidifying TiAl alloys by the proper control of the alloy composition and process parameters. Microstructural observation showed that the billet mainly consists of fine and equiaxed γ grains and a small amount of β phase. The tensile properties of the multi-directional forged alloy were also significantly improved, due to microstructure refinement. The ultimate tensile strength (UTS) and elongation (δ) at room temperature were 689.4 MPa, and 0.83%, respectively. The alloy exhibits excellent ductility at 700 °C. When the temperature was increased to 700 °C, the UTS decreased to 556 MPa and δ increased to 5.98%, indicating that the alloy exhibits excellent ductility at 700 °C. As the temperature further increased to 750 °C, δ dramatically increased to 46.65%, indicating that the ductile-brittle transition temperature of the alloy is between 700 °C and 750 °C.