The hygroscopic nature of wood limits the use of wood thermoplastic composites (WTC) in outdoor industrial and domestic applications. To reduce this tendency, red balau saw dust was heat treated at 180 and 200°C for 1 h and compounded with Low Density Poly(ethylene) (LDPE) into 20 and 37 wt% and then molded into test specimens by injection molding. Samples were immersed in distilled water at room temperature for 4 months. Heat-treated wood composites showed remarkable water resistance relative to untreated ones. Wood composites made from wood treated at 180 and 200°C exhibited almost similar water absorption pattern. Reduced water absorption of heat-treated wood composites relative to untreated ones indicates that heat treatment has resulted in a degree of modification of the wood. Most of the composites displayed the Fickian mode of water absorption with n values close to 0.5. Also, the diffusion coefficient reduced with wood content in untreated wood composites due to interaction of water with the polar groups in wood through hydrogen bonding. Untreated wood composites exhibited poorer mechanical properties with water immersion as a result of degradation due to moisture. The mechanical properties of the heat-treated wood composites were not adversely affected with water absorption. Therefore, heat treatment can reduce the proneness to water absorption in WTCs and alleviate the detrimental effects on mechanical properties.
Kenaf fiber/high-density polyethylene/maleic anhydride (MA)-compatibilized composites were melt mixed in a twin-screw extruder and molded using injection molding machine. Physicothermal properties of the composites were studied at different percentages of compatibilizer contents using various techniques. The addition of 8% compatibilizer into 8.5 and 17.5 wt% fiber content improved the adhesion and tensile strength by 14.5% and 13.6%, respectively. Compatibilized samples exhibited higher peak load and fracture energy on impact testing compared to the samples without maleic anhydride compatibilizer. The effect of the addition of maleic anhydride compatibilizer on peak load and fracture energy was observed to be at its highest at 8%. Differential scanning calorimetric measurements revealed that the melting enthalpy and degree of crystallinity of composites increased with increasing compatibilizer content up to 8% and then decreased at 12% compatibilizer content. Dynamic mechanical analysis showed that the storage modulus of composites was increased, but the loss modulus and tangent delta were decreased after the addition of compatibilizer. This indicates that compatibilized composites produced have improved toughness and reduced stiffness.
Gmelina arborea sawdust was chemically modified using 4% and 8% concentrations of NaOH solution for 30 and 90 minutes soaking times. The influence of this modification on the chemical composition and thermal properties of samples were investigated. Chemical characterization of samples revealed that the percentage content of hemicellulose decreased from 24.5% in the unmodified sample to 20.8%, 17.6% and 15.2% in samples soaked in 4% NaOH solution for 90 minutes, 8% NaOH for 30 and 90 minutes respectively. The amount of lignin decreased from 25.0% in unmodified samples to 19.0% when the sample was treated with 8% NaOH for 90 minutes. A moisture content of 9.0% and 2.5% were recorded in unmodified and sample treated with 8% NaOH for 90 minutes respectively. However, the cellulose content increased from 38.1% in unmodified sample to 60.1% when the sample was treated with 8% NaOH for 90 minutes. The percentage weight loss increased as concentration and modification time increased. Functional groups analysis by Fourier Transform Infrared Spectroscopy (FTIR) showed evidence of reduction in OH and removal of C=O groups associated with the wood polymers after chemical modification. Thermogravimetric analysis revealed that samples treated with 4% NaOH for 90 minutes presented the highest onset and peak degradation temperatures of 274.0°C and 372.1°C respectively. From these results, it can be concluded that modification with 4% NaOH solution for 90 minutes imparted a significant improvement on the thermal stability of Gmelina arborea sawdust.