The external skeleton, frustule, of a diatom is composed of hydrous amorphous silica and amino acids. In this study, the structural changes in the frustule of Chaetoceros calcitrans after thermal treatment up to 1200 °C were investigated using X-ray diffraction and attenuated total reflection infrared spectroscopy and Raman spectroscopy. Their structural changes after thermal treatment give important information to elucidate the unheated structure of the frustule and its crystallization process. In addition, this study is almost the first report to discuss the structure of diatom frustule in detail with Raman spectrum. The unheated structure of the frustule has the relatively ordered and dominant six-membered ring structure made of SiO4 tetrahedra. The sample heated at 800 °C has the more ordered six-membered ring structure observed in quartz or cristobalite. Water molecules and silanol (Si–OH) included in the frustule are dehydrated at this temperature. This dehydration may promote the formation of ordered and polymerized structure. The structure of the frustule after heating at 1200 °C is similar to that of low-cristobalite. However, additional heating is required for complete crystallization.
The nanostructure (atomic-scale structure) and water species in the body frame and spicules of the marine glass sponge, Euplectella aspergillum, collected from the sea floor around Cebu Island was characterized in detail by thermogravimetric differential thermal analysis, nuclear magnetic resonance spectroscopy, Raman and infrared spectroscopies, and X-ray diffraction method. The structural features of the nanostructure in the body frame and spicules were essentially similar to each other, although these were different from those of inorganic amorphous silica materials, such as silica gel and silica glass. In addition, the averaged short and medium range structures of the sponge may be similar to those of tridymite. The water content and water species included in the body frame and spicules were almost the same. More than half of the contained water was physisorbed water molecules, and the rest was attributed to Q3 and Q2 silanol groups. Most of the water species may be present at the surface and involved in hydrogen bonding.
Structural changes in silica gel after compression to 5 GPa and 100 C for one hour were investigated using Raman and IR spectroscopies and X-ray diffraction measurements. The non-powdered silica gel sample was entirely crystallized to coesite under these experimental conditions, showing that the crystallization of silica gel to coesite can be readily achieved in spite of the low temperature conditions and short duration. This behavior may result because the average structure of silica gel is dominated by fourmembered rings of SiO4 tetrahedra, there is a less-polymerized network structure due to the presence of silanol (Si-OH), and larger ring structures, such as 6- and 8-membered rings, of SiO4 tetrahedra are disrupted by water molecules under pressure. These properties may lead to successive polymerization and reconstruction of the SiO4 tetrahedra in the bulk silica-gel sample, enabling the easy formation of the coesite-like network structure. This shows the importance of the contribution of silanol and water molecules for coesite formation.
26 March 2016 in Physics and Chemistry of Minerals