Aleksandra Patarić

Dr. Aleksandra Patarić

orcid

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
17 September 2024 in Crystals
Verified
Journal Article
Open access
PDF file
MDMile Djurdjevic
Mile Djurdjevic
Srecko ManasijevicSrecko Manasijevic
Srecko Manasijevic
APAleksandra Patarić
Aleksandra Patarić
Srecko StopicSrecko Stopic
Srecko Stopic
MMMarija Mihailovic
Marija Mihailovic
The demand for high-performance Al–Si casting alloys is driven by their mechanical properties, making them popular in automotive, aerospace, and engineering industries. These alloys, especially hypoeutectic Al–Si–Mg, offer benefits like high fluidity, low thermal expansion, and good corrosion resistance. Silicon and magnesium primarily define their microstructure and mechanical properties. Silicon enhances fluidity, while magnesium improves strength and fatigue resistance. However, challenges like shrinkage porosity persist during solidification. Understanding solidification feeding regions is crucial, influenced by factors such as chemical composition, solidification characteristics, and casting design. This study investigates magnesium’s influence on feeding ability in hypoeutectic Al–Si7–Mg alloys through experimental tests. Increasing magnesium content from 0% to 0.6% affects the interdendritic and burst feeding regions. This could impact shrinkage porosity formation. The “Sand Hourglass” test results indicate a rise in porosity levels with higher magnesium content, which is linked to the narrowing of interdendritic channels and the formation of magnesium-rich intermetallic compounds. These changes hinder the liquid metal flow, worsening shrinkage porosity. Therefore, magnesium’s role in expanding the interdendritic region is a key factor in developing porosity in cast hypoeutectic Al–Si7–Mg alloys. This study highlights that porosity levels increase from 0% in magnesium-free Al–Si7 to 0.84% in Al–Si7–Mg0.6, underscoring magnesium’s significant impact on the occurrence of porosity in these alloys.

30 September 2017 in Metallurgical and Materials Engineering
Verified
Journal Article
Open access
PDF file
BMBranislav Radomir Marković
Branislav Radomir Marković
DMDragan Manasijević
Dragan Manasijević
NTNadežda Talijan
Nadežda Talijan
MSMiroslav Sokic
Miroslav Sokic
NSNada Strbac
Nada Strbac
MBMladen Dobrivoje Bugarčić
Mladen Dobrivoje Bugarčić
The Bi–Cu–Ni ternary system belongs to the group of potential Cu-Ni-based advanced lead-free solder materials for high temperature application. The paper shows results of the thermodynamic calculations using general solution model along the line with the molar ratio of Cu: Ni = 1:1. The experimental part shows thermal, structural, electrical and mechanical properties based on differential scanning calorimetry (DSC), scanning electron microscopy with energy dispersive spectrometry (SEM-EDS), electroconductivity and hardness measurements of the alloys selected in the section from bismuth corner with molar ratio Cu: Ni = 1:1, Cu: Ni = 3:1, and Cu: Ni = 1:3.

5 November 2025 in Materials
Verified
Journal Article
Open access
PDF file
APAleksandra Patarić
Aleksandra Patarić
MDMile Djurdjevic
Mile Djurdjevic
Srecko ManasijevicSrecko Manasijevic
Srecko Manasijevic
Srecko StopicSrecko Stopic
Srecko Stopic
MMMarija Mihailovic
Marija Mihailovic
Hypoeutectic Al-Si-Mg alloys are among the most widely used casting materials in the automotive and aerospace industries due to their low density, high strength-to-weight ratio, corrosion resistance, and good castability. A critical challenge during solidification is shrinkage porosity, which arises from insufficient feeding and significantly reduces casting reliability. While the role of silicon in altering the phase diagram of Al-Si-Mg alloys is well-understood, its direct impact on feeding behavior has not been previously quantified in detail. In this study, the influence of silicon content (5–9 wt.%) on feeding ability was systematically investigated using thermal analysis (TA). By analyzing cooling curves, first derivatives, and ΔT curves, key solidification temperatures, including the liquidus, dendrite coherency, rigidity, and solidus, were precisely identified. For the first time, these data were used to quantitatively define all five feeding regions (liquid, mass, interdendritic, burst, and solid feeding) as a function of silicon content. The results demonstrate that increasing the Si content decreases the liquidus and dendrite coherency temperatures, raises the rigidity and solidus temperatures, and shortens the overall feeding ranges, particularly the interdendritic region (~32 °C reduction). This novel TA-based quantification of feeding regions provides insights that extend beyond classical phase diagram interpretation. The findings confirm that higher Si contents improve feeding ability by narrowing the freezing range and reducing the risk of porosity, while also providing a unique dataset for validating casting simulation software. The results also confirm that increasing the silicon content enhances feeding ability and improves castability by narrowing the freezing range and promoting more uniform solidification in Al-Si-Mg alloys. The study therefore bridges fundamental solidification science with industrial practice, supporting improved alloy design and defect control in Al-Si-Mg castings.


1 January 2025
Verified
Conference Paper
Open access
PDF file
TRTKoral335Karlo Raic
TKoral335Karlo Raic
MĐMile Đurđević
Mile Đurđević
Srecko ManasijevicSrecko Manasijevic
Srecko Manasijevic
APAleksandra Patarić
Aleksandra Patarić
MMMarija Mihailovic
Marija Mihailovic
The objective of this study is to develop statistical relationships that will enable the quantification of non-metallic inclusion content in continuously cast low-carbon, aluminum-killed deep-drawing steel in situations where standard techniques make metallographic control challenging or impossible. Further considerations can be focused on predicting the model of the size distribution curve after the quantitative characterization of non-metallic inclusions in steel is completed. So, the potential of reconstructing the entire content of non-metallic inclusions in steel will be estimated, and the influence of limiting factors can be assessed.

26 May 2025 in Metallurgical & Materials Engineering Congress of South-East Europe
Verified
Journal Article
Closed access
MDMile Djurdjevic
Mile Djurdjevic
Srecko ManasijevicSrecko Manasijevic
Srecko Manasijevic
APAleksandra Patarić
Aleksandra Patarić
MMMarija Mihailovic
Marija Mihailovic
RRRadomir Radisa
Radomir Radisa
Latent heat of cast hypoeutectic aluminum alloys is commonly measured using Differential Scanning Calorimetry (DSC) or calculated using software packages (Thermo-Calc, JMatPro, FactSage) as well as applying cooling curve analysis (Thermal analysis technique). This study used the DSC method to comprehensively evaluate the accuracy of calculated latent heat for a specific AlSi7Cu1 alloy, considering its solidification under different cooling conditions. The alloy was analyzed under three distinct cooling/heating rates: 6, 10, and 50 °C/min. The commercial software packages (Thermo-Calc, JMatPro, and Fact Sage) and thermal analysis techniques (Newtonian, Fourier, and Energy balance methods) were used to calculate the investigated alloys' latent heat. The results obtained show good agreement between the measured and calculated values. Higher cooling rates, such as 50 °C/min, resulted in a reduced latent heat release compared to slower rates, such as 10 °C/min and 6 °C/min.