High quality nanojunctions are known to effectively improve the conductivity and structural robustness of ultraporous nanoparticle networks, surpassing the performance of natural van der Waals interfaces. Nevertheless, the traditional approach of forming these junctions by thermal annealing is incompatible with thermolabile polymers and slender metal electrodes found in modern wearable technologies. Herein, we present a low temperature, solvent vapor‐based method to rapidly elicit high‐quality metal‐oxide nanojunctions in a fast, effortless, inexpensive, and easily scalable process; capable of generating necked interparticle interfaces in a matter of minutes. When applied to ultraporous‐based ZnO Ultraviolet (UV) photodetectors, the vapor‐tailoring process produces an incredible 128,000‐fold improvement in responsivity (6.6 A.W−1) over untreated structures (51.2 µA.W−1), and a 5300‐fold improvement in responsivity over thermally annealed structures; all while maintaining exceptionally low dark currents of 140 pA at a low bias voltage of 1 V. Most importantly, the exceptional performance enabled by room temperature synthesis suggests high potential adaptability of this process toward wearable UV sensors, shedding lights on the strategy of modifying weakly bonded porous nanostructures for improved physical properties.
15 March 2025 in Journal of the Japan Society of Powder and Powder Metallurgy
Previous studies on the ductility of Ti–O alloys have reported two contrasting behaviors—brittleness and high ductility—yet the critical factors required to achieve high ductility remain unclear. In this study, we investigated the effects of oxygen content and microstructure on the tensile properties of cast Ti–O alloys containing 0.21–0.96 wt% oxygen. The alloys were subjected to homogenization heat treatment followed by hot extrusion or hot rolling to evaluate the influence of oxygen segregation and grain refinement on their ductility. Homogenization eliminated oxygen segregation, leading to improved elongation in alloys with oxygen contents up to 0.59 wt%. Furthermore, thermomechanical processing refined the grain structure and introduced prismatic textures, enabling a remarkable recovery of ductility even in alloys with oxygen contents up to 0.96 wt%. Notably, the extruded alloy exhibited an elongation exceeding 25% at 0.82 wt% oxygen while achieving an ultimate tensile strength (UTS) above 1000 MPa. A systematic investigation of alloys with controlled oxygen content and grain size revealed that, for oxygen levels above 0.4 wt%, fine-grained microstructures exhibited high ductility, whereas ductility decreased once the grain size exceeded a critical threshold. This critical grain size decreased progressively with increasing oxygen content. Fractographic analysis showed that grain boundary cracking dominated in coarse-grained specimens, while fine grains effectively suppressed crack propagation. These findings quantitatively demonstrate that the ductility of Ti–O alloys is governed jointly by oxygen content and grain size and provide a material design strategy for the effective utilization of interstitial elements.