Apparently mundane, amorphous nanostructures of carbon have optical properties which are as exotic as their crystalline counterparts. In this work we demonstrate a simple and inexpensive mechano-chemical method to prepare bulk quantities of self-passivated, amorphous carbon dots. Like the graphene quantum dots, the water soluble, amorphous carbon dots too, exhibit excitation-dependent photoluminescence with very high quantum yield (~40%). The origin and nature of luminescence in these high entropy nanostructures are well understood in terms of the abundant surface traps. The photoluminescence property of these carbon dots is exploited to detect trace amounts of the nitro-aromatic explosive — 2,4,6-trinitrophenol (TNP). The benign nanostructures can selectively detect TNP over a wide range of concentrations (0.5 to 200 µM) simply by visual inspection, with a detection limit of 0.2 µM, and consequently outperform nearly all reported TNP sensor materials.
Excitation-dependent, multicolor emission from different varieties of 0D carbon systems has attracted immense research attention. It is generally accepted that some variants of 0D carbon exhibit excitation dependent emission, while other variants do not. A third variant exhibits both excitation dependent as well as excitation independent emission. In this work we investigate the structure, composition, steady-state emission-excitation and photoluminescence decay dynamics of three distinctly different variants of 0D carbon – amorphous carbon dots (aCDs), graphene quantum dots (GQDs) and nitrogen-doped GQDs (NGQDs). We find that despite significant differences in the structure and composition there is a striking similarity in the excitation energy dependence of the emission characteristics of these three different dots. All of them exhibit excitation energy independent emission below some threshold wavelength (λth), and above this threshold the emission becomes excitation dependent. We also demonstrate that a similar trend is apparent for nearly all variants of 0D carbon reported in the literature. The threshold wavelength correlates well with the excitation wavelength for the most intense emission and the photoluminescence excitation peaks, suggesting a common origin of light emission in these carbon dots. The findings provide important clues for developing a unified general picture for understanding the light emission mechanism in 0D carbon nanostructures.
We report the synthesis of spherical core-shell structures of silicon and silicon oxide by a novel route of forced external oxidation of ball milled silicon. Structural investigations reveal the formation of a crystalline silicon core surrounded by an amorphous oxide shell, with core and shell dimensions varying approximately between 4–10 and 55–170 nm, respectively. The observations suggest partial amorphization of crystalline silicon, invasive oxygen induced passivation of dangling bonds, and formation of different types of defects in the nanocrystalline silicon/silicon oxide core-shell structure, particularly at the interfaces. No detectable photoluminescence (PL) is obtained from the as-milled silicon, but the oxidized core-shell structures exhibit strong room temperature PL, detectable with unaided eye. The peak energy of the PL spectra blueshifts with an increase in excitation energy, with the peak positions varying from 2.24 to 2.48 eV under external excitation ranging from 2.41 to 3.5 eV. The observed PL characteristics are explained in terms of dominant electronic transitions between the localized defect states and quantum confinement induced widened band states.
We report synthesis and luminescent characteristics of core-shell nanostructures of silicon and silicon oxide having two different morphologies—spherical (nanodot) and rodlike (nanorod), prepared by controlled oxidation of mechanically milled crystalline silicon and by exfoliation of the affected layer of porous silicon. Colloidal suspensions of these nanostructures exhibit intense room temperature photoluminescence (PL), detectable with the unaided eye. PL band peak energies of the colloidal suspensions formed from porous silicon are blue shifted by compared to the as-prepared films on silicon substrate. In addition, PL spectra of all the colloidal suspensions blueshift with increase in excitation energy but the PL peaks of as-prepared porous silicon are independent of excitation. However, shape of the nanocrystals (spherical or rodlike) is found to have little effect on the emission spectra. These observations are explained in terms discretization of phonon density of states and electronic transitions involving surface defect states and quantum confinement induced widened band states.
We report the synthesis of luminescent, free standing silicon quantum dots by dry and wet etching of silicon and silicon oxide core/shell nanostructures, which are synthesized by controlled oxidation of mechanically milled silicon. Dry and wet etching performed with CF(4) plasma and aqueous HF, respectively, result in the removal of the thick oxide shell of the core/shell nanostructures and affect an additional step of size reduction. HF etch is capable of producing isolated, spherical quantum dots of silicon with dimensions ∼ 2 nm. However, the etching processes introduce unsaturated bonds at the surface of the nanocrystals which are subsequently passivated by oxygen on exposure to ambient atmosphere. The photoluminescence spectra of the colloidal suspensions of these nanocrystals are characterized by double peaks and excitation dependent shift of emission energy. Comparison of the structural, absorption and luminescence characteristics of the samples provides evidence for two competing transition processes--quantum confinement induced widened band gap related transitions and oxide associated interface state mediated transitions. The results enable us to experimentally distinguish between the contributions of the two different transition mechanisms, which has hitherto been a challenging problem.