The Cu undercut is a recently discovered new defect generated in the wet stripping process of MoNb/Cu gate stacked electrodes for thin-film transistors (TFTs). The formation mechanism and preventive strategy of this defect were identified and investigated in this paper. The impact of stripper concentration and stripping times on the morphology and the corrosion potential (Ecorr) of Cu and MoNb were studied. It is observed that the undercut is Cu tip-deficient, not the theoretical MoNb indentation, and the undercut becomes severer with the increase in stripping times. The in-depth mechanism analysis revealed that the abnormal Cu undercut was not ascribed to the galvanic corrosion between MoNb and Cu but to the local crevice corrosion caused by the corrosive medium intruding along the MoNb/Cu interface. Based on this newly found knowledge, three possible prevention schemes (MoNiTi (abbreviated as Mo technology development (MTD) layer/Cu), MoNb/Cu/MTD, and MoNb/Cu/MoNb) were proposed. The experimental validation shows that the Cu undercut can only be completely eliminated in the MoNb/Cu/MTD triple-stacked structure with the top MTD layer as a sacrificial anode. This work provides an effective and economical method to avoid the Cu undercut defect. The obtained results can help ensure TFT yield and improve the performance of TFT devices.
The electrodes of thin film transistors (TFTs) have evolved from conventional single Cu layers to multi-layered structures formed by Cu and other metals or alloys. Different etching rates of various metals and galvanic corrosion between distinct metals may cause etching defects such as rough or uneven cross-sectional surfaces of stacked electrodes. Therefore, the etching of stacked electrodes faces new challenges. CD Bias and profile angle (PA) are two main performance indicators for the wet etching of TFT electrodes. Adjusting CD Bias and PAs quantitatively and evaluating their stability accurately is crucial to ensure the performance and yield of TFTs. In this work, the bilayer MoNb/Cu-stacked electrodes with different MoNb thicknesses and the MoNb/Cu/MTD triple-layered electrodes were prepared, and the influence of MoNb thickness and stacked structure on the CD Bias and PAs was investigated. It is found that in the H2O2-based etchant, the order of corrosion potential is EMTD < EMoNb < ECu; both MoNb/Cu and Cu/MTD will form a primary cell with MoNb or MTD as the anodes. The CD Bias and PAs of the MoNb/Cu bilayer structure also increase with MoNb thickness, but those of the MoNb/Cu/MTD triple-layered structure decrease with the introduction of the top MTD film. Finally, regression equations between CD Bias or PA and etching parameters were established based on the results of uniform experiments, and the 95% confidence intervals for CD Bias and PA were proposed after the Monte Carlo simulation. These obtained results provide a basis for quantitative adjustment of CD Bias and PA and precise control of etching stability.
Thin-film transistors (TFTs) based on quinary indium-gallium-zinc-tin oxide (IGZTO) were fabricated via radio frequency (RF) magnetron sputtering. The impact of vacuum annealing temperatures (25–450 °C) on the microstructural and optoelectrical properties of films and TFTs was systematically investigated. All IGZTO thin films are amorphous and transparent, with optical bandgaps ranging from 3.22 eV to 3.63 eV. The one annealed at 350 °C exhibited the smoothest surface. The carrier concentrations and Hall mobilities of IGZTO films vary with the annealing temperature in the range of 7.44 × 1018 ~ 6.37 × 1019 cm−3 and 20.89~35.53 cm2·V−1·s−1, respectively. Oxygen vacancies () are considered the major origin of the conductivity of IGZTO films, and their evolution with annealing temperatures was elucidated. The TFT annealed at 350 °C achieved a saturation mobility (μsat) of 19.7 cm2 V−1 s−1, threshold voltage (VTH) of 4.72 V, subthreshold swing (SS) of 0.56 V dec−1, and Ion/Ioff of 8.1 × 107, but TFTs annealed at other temperatures show no switching behaviour. TCAD simulations indicate that vacuum annealing elevates density, especially at the film surface; the switching failure at 150 °C and 450 °C is attributed to the pronounced structural disorder expressed by large characteristic slope energies of tail states, while the failure at 250 °C is due to excessive density. This work may provide useful guidance for the performance optimisation of IGZTO film and TFTs via annealing.